The concrete represent materials/rock that is yielded by mixing smooth aggregate (sand), harsh aggregate (gravel), water andportland cement according to Regulation of Reinforced Concrete Indonesia (PBI) 1971 NI-2. Detergent concentraton (LAS) andDiesel fuel, LAS + Diesel fuel was added in each treatment of 0%; 1 ; 2,5 ; 5% to mixed water until attain minimum standard ofdepress strength according to SNI. From result of research revealed that content of LAS 0,3 % aftarned depress strength concreteequal to 23,578 Mpa at 7 day and 28,654 Mpa at 28 day according to minimum requiretment of SNI with ercentage equal to 90,24 %and 89,67 %. With Diesel fuel content 5 % afterned depress concrete strength equal to - 23,536 Mpa at 7 day and 28,717 Mpa at 28days according to minimum requitement of SNI with percentage equal to 90,08 % and 89,87 %. With mixture content of LAS andDiesel of fuel 0,2% afterned depress concrete strength equal to 23,610 Mpa at 7 days and 28,698 Mpa at 28 days according tominimum reqirement of SNI with percentage equal to 90,36 % and 89,81 %.
                        
                        
                        
                        
                            