Welded joints in ST 41 low-carbon steel commonly show unpredictable hardness variation across the Heat Affected Zone (HAZ), and although Post-Weld Heat Treatment (PWHT) and multipass welding are each known to influence this variation, their combined effect on ST 41 has not been systematically examined. This study evaluates how weld pass count (2, 3, and 4 layers) and PWHT at 590 °C interact to affect HAZ and weld metal hardness and microstructure. SMAW welded specimens with E6013 electrodes (Ø3.2 mm) at 100 A. PWHT was applied for 30 minutes, followed by furnace cooling. Dye penetrant testing confirmed all 18 joints were free from critical defects, with minor porosity in three specimens within ASME limits. Without PWHT, the highest mean weld metal hardness was 266.38 HV (4-pass), with an individual HAZ peak of 388.10 HV in specimen T42; the lowest non-PWHT HAZ hardness (239.29 HV) occurred in the 3-pass group. After PWHT, HAZ hardness fell across all pass counts, most markedly in the 3-pass group (196.09 HV, an 18% reduction), although the reduction did not reach statistical significance at the sample size tested. Microstructural examination showed a consistent shift from fine pearlite with poorly defined grain boundaries before PWHT to coarser, more homogeneous ferrite-pearlite afterwards, corresponding with the hardness trend. These results suggest that combining a three-pass sequence with PWHT at 590 °C offers the most favourable hardness reduction for ST 41 weld joints, a finding that warrants confirmation with a larger specimen set.
Copyrights © 2026