Polycarbonate (PC) is widely used in engineering applications because of its excellent mechanical properties, dimensional stability, and thermal resistance. However, repeated thermal processing during mechanical recycling may alter its thermal behavior, while quantitative information regarding thermal-response changes after multiple reprocessing cycles remains limited. This study aimed to investigate the effect of repeated reprocessing cycles on the thermal response of recycled polycarbonate using Differential Scanning Calorimetry (DSC). The contribution of this study is the systematic evaluation of how DSC-observed thermal responses evolved across 3, 6, and 9 controlled reprocessing cycles, enabling relatively small early-cycle changes to be distinguished from the more pronounced shifts observed at higher reprocessing histories. Virgin PC and recycled PC samples were prepared through repeated remelting and reprocessing. Thermal characterization was performed using DSC according to ASTM D3418 and ISO 11357-2. The glass transition temperature (Tg) and DSC-observed degradation-related thermal event temperature (Td) were evaluated to assess changes in thermal response associated with repeated reprocessing. The results showed that Tg gradually decreased from 149.47 °C for virgin PC to 148.53 °C, 146.79 °C, and 145.17 °C after 3, 6, and 9 cycles, respectively. Td initially increased slightly from 451.59 °C to 455.33 °C after 3 cycles, then decreased to 435.13 °C and 429.29 °C after 6 and 9 cycles. Overall, repeated reprocessing was associated with gradual shifts in thermal response, reflected by changes in Tg and DSC-observed degradation-related thermal events.
Copyrights © 2026