This study maps waste and identifies the determinants of inefficiency in the lost-PLA metal casting practicum and examines the learning outcomes associated with a waste-aware practicum developed from that map. A mixed-method design was used. The first phase involved 66 students completing a 40-item questionnaire on twelve practicum stages; categorical durations were converted into minutes and each stage was classified as value-added, non-value-added, or necessary non-value-added. The second phase used a non-equivalent control group design with 85 students, 28 in the control class and 57 in two treatment classes, over four meetings. Learning outcomes were measured with a 20-item test administered one month apart. Analysis employed bottleneck ranking, the seven-waste framework, Spearman correlation with Holm correction, normalised gain, Kruskal-Wallis, and Mann-Whitney tests. Waiting dominated the measured waste profile at 64.0%, concentrated in machine and furnace queues. Pattern design and printing was the main bottleneck at 57.3 minutes against a required pace of 45 minutes per unit, of which 38.8 minutes were waiting. Finishing, cooling, and melting were the strongest determinants of perceived inefficiency. The treatment classes reached a normalised gain of 0.723 against 0.226 in the control class. Waste in the casting practicum is structural rather than individual.
Copyrights © 2026