Coil Spring Failure Analysis Reviewed from Residual Stress, Crytal Orientation, and Texture Andoko Andoko; Rifqi Ryandi Dwi Ananto; Heru Suryanto; Femiana Gapsari; Maykel Manawan
Automotive Experiences Vol. 6 No. 3 (2023)
Publisher : Universitas Muhammadiyah Magelang

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.31603/ae.9803

Abstract

Crystal defects can be identified through the crystallographic characteristics of crystal orientation (lattice), microstrain, and texture. Identification of crystal defects on the atomic scale through crystallography is very important in analyzing the mechanism of material properties due to the influence of dislocations. The slip mechanism is analyzed to minimize coil spring failure. This study aims to analyze the causes of coil spring failure based on crystallography. XRD testing was carried out for analysis of residual stress, crystal orientation, and texture using MAUD 2.94 version software. Hardness testing was carried out on the surface of the coil spring with locations near and far from the fracture using micro Vickers. The macro fracture morphology was analyzed using a DSLR camera and the micro fracture morphology was analyzed using SEM. The XRD result shows that the coil spring material has a tensile residual stress value of "202.4 ± 15.9 MPa" with the resulting crystal orientation showing the hkl (100), (200), (211), (200) fields. The plane (200) has a texture characteristic that is oriented towards the Rolling direction along the spring axis. Texture oriented towards Rolling Direction can be shown with a maximum probability value of 1.191. A high probability will have an impact on the presence of material surface defects. Surface defects are indicated by the presence of pit corrosion on micro and macro fracture morphology observations. The pit corrosion defects that occur in the failed coil springs are the beginning of the formation of crack initiation and cause stress concentration. The stress concentration will increase with loading and cause crack propagation.
Optimized deposition parameters for titanium nitride coatings: Enhancing mechanical properties of Al 6011 substrates via DC sputtering Margono Margono; Djarot Bangun Darmadi; Femiana Gapsari; Teguh Dwi Widodo; Muhammad Kozin; Prabowo Puranto; Muhammad Prisla Kamil; Diah Ayu Fitriani; Siti Amalina Azahra; Wiwien Andriyanti
Mechanical Engineering for Society and Industry Vol. 4 No. 2 (2024)
Publisher : Universitas Muhammadiyah Magelang

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.31603/mesi.12266

Abstract

The growing demand for advanced coatings in industries such as aerospace and automotive necessitates materials with superior hardness, wear resistance, and thermal stability. Despite advancements in ternary coatings, research on binary Titanium Nitride (TiN) coatings remains limited, particularly in optimizing deposition parameters for lightweight aluminum substrates. This study aims to investigate the effects of sputtering parameters, specifically Ar:N₂ gas ratios and deposition durations, on the mechanical properties of TiN coatings on Al 6011 substrates. The optimized conditions (70Ar:30N₂ gas ratio and 60-minute deposition) yielded a 165% increase in surface hardness (88.92 HV) and a 54% reduction in wear rate compared to untreated samples. XRD and SEM analyses confirmed the dense microstructure and strong (200) phase orientation contributing to these enhancements. This research highlights a cost-effective and scalable approach to improving the performance of aluminum alloys, bridging the gap between fundamental studies and industrial applications.