Pengaruh Penggunaan  Superplasticizer  Terhadap Slump Flow  Dan Kuat Tekan Beton Sarah Annisa Muchtar; Sudirman Sudirman; Nafsiah Aswawi
Jurnal Ilmiah Ecosystem Vol. 26 No. 2 (2026): Ecosystem Vol. 26 No 2, Mei - Agustus Tahun 2026
Publisher : Lembaga Penelitian dan Pengabdian kepada Masyarakat

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.35965/eco.v26i2.9847

Abstract

Fasilitas infrastruktur seperti jembatan dengan bentang panjang dan lebar, bangunan gedung bertingkat tinggi (terutama untuk kolom dan beton pracetak), landasan pacu dan fasilitas lain, memerlukan beton mutu K-300. Yang dimaksud dengan beton mutu K-300 pada penelitian ini adalah beton yang dipersiapkan berdasarkan SNI 03-2834-2000. Beton mutu tinggi dicirikan dengan pori-pori yang kecil dan padat. Penelitian ini bertujuan untuk mengetahui pengaruh penambahan superplasticizer terhadap kuat tekan beton sehingga dapat mengurangi penggunaan semen. Metode pengumpulan data meliputi analisis gradasi agregat, mix design dan uji kuat tekan saat umur beton 28 hari pada beton K-300. Dari serangkaian pengamatan yang dilakukan, penambahan superplasticizer dihasilkan nilai kuat tekan normal 26,61 Mpa, SP 1,75% 27,27 Mpa, SP 2% 31,64 Mpa dan SP 2,25% 32,03. Hasil ini memberikan indikasi bahwa penambahan superplasticizer berpengaruh signifikan terhadap kuat tekan beton mutu K-300. Infrastructure facilities such as long and wide span bridges, high-rise buildings (especially for columns and precast concrete), runways and other facilities, require K-300 quality concrete. What is meant by K-300 quality concrete in this study is concrete prepared based on SNI 03-2834-2000. High quality concrete is characterized by small and dense pores. This study aims to determine the effect of superplasticizer addition on concrete compressive strength so as to reduce cement usage. Data collection methods include aggregate gradation analysis, mix design and compressive strength test at 28 days of concrete age on K-300 concrete. From a series of observations made, the addition of superplasticizer produced a normal compressive strength value of 26.61 Mpa, SP 1.75% 27.27 Mpa, SP 2% 31.64 Mpa and SP 2.25% 32.03. These results indicate that the addition of superplasticizer has a significant effect on the compressive strength of K-300 concrete.