FLEXURAL STRENGTH OF LIP CHANNELS COLD FORMED STEEL BEAM IN BACK-TO-BACK ARRANGEMENT WITH A VARIETY OF LENGTHS Nindyawati Nindyawati; M. Mirza Abdillah Pratama; Husnik Maulidya Tungga Dewi
Bangunan Vol. 27 No. 1.1 (2022): BANGUNAN EDISI KHUSUS MARET 2022: Pengembangan Material dan Metode Konstruks
Publisher : Universitas Negeri Malang

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17977/10.17977/um071v27i1.12022p23-36

Abstract

Optimization of cold-formed steel construction materials in the form of merging two individualchannel into built up back-to-back channel. The use of cold-formed steel is increasingly applicable withvarying lengths used. Therefore, it is necessary to research the effect of variations in beam span lengthaffect the flexural strength of cold-formed steel beams arranged back to back. This study aims todetermine the load, deflection, and failure mode of back-to-back C channel beam with variations in beamspan length. The research uses quantitative methods through a laboratory experimental approach. Theresults of the study can be concluded as follows: (1) A load of back-to-back cold-formed steel beams hasdecreased with an increase in the length of the beam span in each variation code test specimen. Thedecrease in load compared to the shortest span length of 90 cm for the lengths of 120, 210, 240 cm are10,90%, 51,12%, and 62,39% respectively. The decrease in actual load is caused by a reduction offlexural rigidity, the presence of stress concentrations at the loading point that prevent the load from beingproperly distributed to the support, and the instability of the back-to-back or open sections, whichincreases as the length of the beam span increase. (2) Deflection of the beam due to transverse loadswhich act on back-to-back cold-formed steel beams increases as the span length increases for eachvariation code test spesimen. The beam deflection compared to the shortest span length of 90 cm for thelengths of 120, 210, and 240 cm increased by 17,26%, 73,11% dan 103,3% respectively. The decrease inbeam stiffness due to increased length of the beam span with a constant spreader beam size, which resultsin increased distance between the loading point and the support, is what causes the rise in verticaldeflection of the beam. The deflection that occurs in each length variation code exceeds the maximumdeflection limit, so it is necessary to take into consideration of the load applied to the back to back coldformed steel beam. (3) The failure modes that occured in the back-to-back cold-formed steel beam in eachvariation of the span length during the flexural test had the same failure, namely flange local buckling,distortional buckling, and lateral torsional buckling. The difference in failure modes among C channels inthe back-to-back beam was observed and there is an interaction of local buckling, distortional, and lateraltorsional buckling failure modes in one of C channel, while the other C channel only experiences lateraltorsional buckling
EXPERIMENTAL STUDY OF FLEXURAL CFS BEAM DOUBLE CHANNEL FACE TO FACE IN LENGTH VARIATIONS Cahyana Alvyonika; Nindyawati Nindyawati; M. Mirza Abdillah Pratama
Bangunan Vol. 27 No. 1.1 (2022): BANGUNAN EDISI KHUSUS MARET 2022: Pengembangan Material dan Metode Konstruks
Publisher : Universitas Negeri Malang

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17977/10.17977/um071v27i1.12022p37-49

Abstract

e application of cold formed steel material as a structural element of buildings has begun tobe considered because the material is strong and light. The capacity of single-section cold formed steelcan be increased by combining the sections. There is less research on cold formed steel beams thancolumns. Research on the failure pattern of cold formed steel with variations in length has not been donebefore. This study aims to obtain the value of flexural capacity, deflection at maximum load, and collapsepattern of cold formed steel beams. The research was conducted experimentally on a simple supportedface to face cold formed steel beam (roll-joint) by applying a four-point bending load to obtain failure dueto pure bending. The results of this study indicate, the longer the face to face cold formed steel beam, thesmaller the value of the load capacity that can be held and the greater the deflection value that occurswhen the maximum transverse load is the Double cold formed steel beam arranged face to faceexperiencing instability from the beginning of loading so that the pattern failure that occurs in the form oflateral torsional buckling. Beam instability increases with increasing beam span length. A cold formedsteel beam with a span length of 700 mm has a load capacity of 6.4 kN and a deflection of 14.5 mm. Thefailure pattern that occurs is in the form of lateral torsional buckling with a torque value of 0.74° and alateral deflection of 0.12 mm. Cold formed steel beams with a span length of 1300 mm are capable ofwithstanding a maximum load of 4, 8 kN and deflection at maximum load of 32.37 mm. The beamexperienced a failure pattern in the form of lateral torsional buckling with a rotation of 1.57° and a lateraldeflection of 0.74 mm. The cold formed steel beam with a length of 3900 mm has a rated load capacity of1.7 kN and a deflection of 91.49 mm. The failure pattern that occurs when the maximum load is in theform of torsional buckling of 4.02° and lateral deflection of 2.41 mm. The load capacity of the coldformed steel beam with a span length of 4300 mm is 1.4 kN and the deflection at maximum load is 99.43mm. The beam experienced a lateral torsional buckling failure pattern with a turning angle of 12.56° anda lateral deflection of 4.84 mm. The cold formed steel beam with a length of 3900 mm has a rated loadcapacity of 1.7 kN and a deflection of 91.49 mm. The failure pattern that occurs when the maximum loadis in the form of torsional buckling of 4.02° and lateral deflection of 2.41 mm. The load capacity of thecold formed steel beam with a span length of 4300 mm is 1.4 kN and the deflection at maximum load is99.43 mm. The beam experienced a lateral torsional buckling failure pattern with a turning angle of12.56° and a lateral deflection of 4.84 mm. The cold formed steel beam with a length of 3900 mm has arated load capacity of 1.7 kN and a deflection of 91.49 mm. The failure pattern that occurs when themaximum load is in the form of torsional buckling of 4.02° and lateral deflection of 2.41 mm. The loadcapacity of the cold formed steel beam with a span length of 4300 mm is 1.4 kN and the deflection atmaximum load is 99.43 mm. The beam experienced a lateral torsional buckling failure pattern with aturning angle of 12.56° and a lateral deflection of 4.84 mm