CONTROLLED GROWTH OF IRON OXIDE MAGNETIC NANOPARTICLES VIA COPRECIPITATION METHOD AND NaNO3ADDITION. Size controlled magnetic nanoparticle (MNPs) of iron oxide were prepared in the presence of NaNO3 via co-precipitation method followed by HNO3 peptizing according to Massart’s method. The MNPs size were reduced by addition of NaNO3 in varied molarity and at different stage of process. As an end product, stable water-base colloids were formed. XRD pattern analysis using Rietveld method confirmed Fe3O4/γ-Fe2O3 phase formation with nanoscale crystallite size. This crystallite size significantly decrease with NaNO3 addition from 12 nm to smaller than 8 nm, and give end-result of decreasing magnetization as measured by VSM. Langevin fitting of magnetic hysteresis curve also revealed the magnetic core size of nearly the same behaviour. TEM results show bigger value for single magnetic nanoparticle of > 10 nm and < 10 nm for MNPs without and with NaNO3 addition, respectively. However, PSA measurement still trace a low nanoparticle agglomeration of ~ 20 nm, even after surface peptization using HNO3. A possible mechanism is proposed to explain these characteristics formation especially of the MNP’s size. ABSTRAK PENGENDALIAN PENUMBUHAN NANOPARTIKEL MAGNETIK OKSIDA BESI DENGAN METODA KO-PRESIPITASI DAN PENAMBAHAN NaNO3. Nanopartikel magnetik oksida besi dengan ukuran terkendali telah dipreparasi dengan metoda ko-presipitasi dan penambahan NaNO3 serta peptisasi HNO3 mengikuti metoda Massart. Pengendalian ukuran nanopartikel magnetik dilakukan dengan memvariasikan nilai molaritas serta tahapan proses penambahan NaNO3. Hasil analisis pola difraksi sinar-X dengan metoda Rietveld mengkonfirmasi terbentuknya fasa Fe3O4/γ-Fe2O3 dengan penurunan ukuran kristalit dari 12 nm untuk sampel tanpa penambahan NaNO3 menjadi 8 nm setelah penambahan NaNO3. Pengecilan ukuran ini juga teranalisis pada hasil fitting kurva magnetisasi dengan persamaan Langevin serta pengamatan dengan TEM. Namun hasil pengukuran PSA tetap mendeteksi adanya aglomerasi nanopartikel dengan ukuran aglomerat terkecil ~20 nm meski telah dilakukan upaya peptisasi dengan HNO3. Mengacu pada berbagai data karakteristik dan hasil analisis ini, mekanisme pengendalian pertumbuhan ukuran partikel ini dicoba dijelaskan dalam artikel ini.