PREPARASI DAN KARAKTERISASI HIDROKSIAPATIT BERPORI DARI TULANG IKAN Ari Handayani; Sulistioso Giat S; Deswita
Jurnal Sains Materi Indonesia Vol. 14 No. 1 (2012): Jurnal Sains dan Materi Indonesia
Publisher : BRIN Publishing (Penerbit BRIN)

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/jsmi.2012.14.1.4640

Abstract

PREPARASI DAN KARAKTERISASI HIDROKSIAPATIT BERPORI DARI TULANG IKAN.Telah dilakukan pembuatan hidroksiapatit (HAp) berpori dengan bahan dasar limbah tulang ikan dan sebagaibahan porogen kitosan dengan metode kalsinasi pada suhu 1.100 °C selama 5 jam. Analisis termogravimetridilakukan dengan Simultan Thermal Analyzer(STA), identifikasi fasa dilakukan dengan X-Ray Diffractometer(XRD), analisis strukturmikro dengan Scanning Electron Microscope (SEM). Analisis termogravimetrimenunjukkan puncak penurunan berat pada suhu 365,6 °C dan setelah suhu 500 °C tidak terjadi penurunanberat lagi. Identifikasi fasa menunjukkan adanya fasa hidroksiapatit pada tulang ikan mentah dan tulang ikansetelah dikalsinasi pada 1.100 °C selama 5 jam. Hasil SEM menunjukkan strukturmikro berpori antar partikelpada tulang ikan mentah dan setelah kalsinasi 1.100 °C selama 5 jam dengan ukuran partikel sebesar 0,1 µmhingga 1,0 µm. Setelah penambahan kitosan, pori antar partikel yang terbentuk lebih merata dan jelas.
PENGARUH IMPLANTASI ION TITANIUM NITRIDA TERHADAP SIFAT MEKANIK BIOMATERIALAISI 316L Sulistioso Giat S; Soeharto; Dian Ika Rahmawati; Tjipto Suyitno
Jurnal Sains Materi Indonesia Vol. 13 No. 4 (2012): Jurnal Sains dan Materi Indonesia
Publisher : BRIN Publishing (Penerbit BRIN)

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/jsmi.2012.13.4.4750

Abstract

PENGARUH IMPLANTASI ION TITANIUM NITRIDA TERHADAP SIFAT MEKANIK BIOMATERIALAISI 316L. Telah dilakukan analisis sifat mekanik dari material stainless steel AISI 316L yang diimplantasi ion Titanium Nitrida (TiN) dengan variasi waktu implantasi 60 menit,90 menit dan 120 menit. Untuk mengetahui beban maksimum yang diberikan pada sampel pada waktu uji lelah, maka dilakukan uji tarik dengan menggunakan 3 buah sampel sebelum sampel diimplantasi dengan ion TiN. Didapat rata-rata tegangan tarik maksimum adalah 69,543 kgf/mm2 (695,43 MPa), sedangkan rata-rata tegangan luluhnya adalah 63,852 kgf/mm2 (638,52 MPa). Kemudian dilakukan uji lelah (fatique test) untuk melihat pengaruh perlakuan implantasi dengan TiN pada umur lelah dari AISI 316L, menggunakan metode rotating bending. Uji awal dari penentuan umur lelah, dilakukan uji lelah untuk waktu implantasi 0 menit,60 menit, 90 menit dan 120 menit dengan beban 460 MPa. Hasil pengujian, umur leleh sesuai dengan waktu implantasi, adalah 15.567 cycles, 16.050 cycles, 21.950 cycles dan 19.100 cycles. Waktu implantasi yang menghasilkan umur lelah tertinggi adalah 90 menit. Kemudian dilakukan uji umur lelah untuk waktu implantasi 90 menit dengan beban 420 MPa, 440 MPa, 460 MPa dan didapat hasil berturutan sebagai berikut 213.700 cycles, 83.433 cycles dan 21.853 cycles. Hasil uji kekerasan sebagai fungsi dari waktu implantasi 0 menit, 60 menit, 90 menit, 120 menit pada titik terluar adalah : 387 VHN, 440 VHN, 586 VHN dan 674 VHN. Dapat disimpulkan bahwa waktu implantasi untuk mendapatkan umur lelah terbaik adalah 90 menit, tapi untuk kekerasan sampel, semakin lama waktu implantasi maka sampel semakin keras. ABSTRACTIMPLANTATION EFFECT OF TITANIUM NITRIDE (TiN) ION ON MECHANICAL PROPERTIES OF AISI 316L BIOMATERIALS . Mechanical properties analysis of AISI 316L stainless steel, implanted by Titanium Nitride (TiN) ion with varied implantation time of 60, 90 and 120 minutes have been carried out. To determine the maximum load for fatigue test, the tensile test first performed by using 3 pieces of the sample before implanted with TiN. The test results gave the maximum average value of tensile stress of 69.543 kgf/mm2 (695.43 MPa), while the average yield strength is 63.852 kgf/mm2 (638.52 MPa). Fatigue test was then performed to analyze the effect of TiN implantation to fatigue life of AISI 316L, using the method of rotating bending. Initial fatigue test, conducted using 460 MPa load, gave fatigue life of 15,567 cycles, 16,050 cycles, 21,950 cycles and 19,100 cycles for sample with implantation time of 0,60,90 and 120 minutes respectively. These data gave the highest fatigue life for 90 minutes sample. Fatigue test was then continued to perform on this sample with varied load of 420, 440 and 460 MPa which gave the fatigue lifetime value of 213,700 cycles, 83,433 cycles and 21,853 cycles respectively. Hardness test results as at outer point were 387 VHN, 440 VHN, 586 VHN and 674 VHN for sample with implantation time of 0, 60, 90, 120 minutes respectively. It can be concluded thatthe longer the time of implantation, the sample will be harder but the best fatigue life reach at 90 minutes time of implantation.
HIDROKSIAPATIT BERPORI DARI KULIT KERANG Saryati; Sulistioso Giat S; Supardi; Puji Untoro; Bambang Sugeng
Jurnal Sains Materi Indonesia Vol. 13 No. 4 (2012): Jurnal Sains dan Materi Indonesia
Publisher : BRIN Publishing (Penerbit BRIN)

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/jsmi.2012.13.4.4753

Abstract

HIDROKSIAPATIT BERPORI DARI KULIT KERANG. Hidroksiapatit (HAp) Ca10(PO4)6(OH)2 merupakan material keramik bioaktif dengan bioafinitas yang tinggi dan bersifat biokompatibel terhadap tubuh manusia. Hidroksiapatit berpori saat ini sudah menjadi kebutuhan yang mendasar bagi rekonstruksi tulang yang patah atau retak. Sementara banyak limbah kulit kerang yang dapat digunakan sebagai bahan dasar pembuatan HAp untuk diproses lebih lanjut menjadi HAp berpori. HAp berpori dibuat melalui pembuatan komposit HAp-porogen. Telah dilakukan pembuatan hidroksiapatit dari kulit kerang dengan jalan reaksi pengendapan. Kulit kerang diubah menjadi CaO kemudian direaksikan dengan diamonium fosfat dan endapannya dikalsinasi sehingga terbentuk HAp dimana kitosan digunakan sebagai porogen. Hasil yang diperoleh dikarakterisasi dengan X-Ray Diffractometer (XRD) dan Scanning Electron Microscope (SEM). Dari Data XRD terlihat bahwa kemurnian fasa HAp dipengaruhi oleh suhu kalsinasi. Diperoleh untuk HAp murni, suhu kalsinasi tidak lebih dari 700°C. Morfologi permukaan serbuk HAp dan HAp berporogen, tidak terlihat perbedaan yang berarti, tersusun oleh bentuk granular (aglomerasi) dari partikel dengan ukuran berkisar 0,1 µm hingga 1 µm dan membentuk pori-pori dengan ukuran berkisar pada 0,1 µm hingga 1,0 µm. Sementara dalam bentuk pelet, permukaan HAp berporogen terlihat mempunyai pori-pori yang lebih besar dan lebih banyak dari HAp yang tidak berporogen. ABSTRACTPOROUS HYDROXYAPATITE FROM CLAMSHELLS. Hydroxyapatite (HAp) Ca10(PO4)6(OH)2 is a bioactive ceramic material with high bioaffinity and biocompatible to the human body. Porous HAp is now a fundamental requirement for the reconstruction of a broken or fractured bones. There are waste a lot of clamshell waste in Indonesia that can be used as a base for manufacture of Hap and continued into porous HAp. Generally the porous HAp was made through HAp-porogen composite. Have been studied the manufacture of clamshells HAp by precipitation reactions. Clamshells converted into CaO and then reacted with diammonium phosphate and calcinated to form sediment Hap. It was used chitosan as a porogen. The results obtained were characterized by X-Ray Diffractometer (XRD) and Scanning Electron Microscope (SEM). From the XRD data shows that the phase purity of HAp is affected by calcination temperature. The conclusions are that to obtain pure HAp calcination temperature not exceeding 700°C. Surface morphology of HAp and porous HAp powder, look no significant difference, composed of granular forms (agglomeration) of particles with a size range from 0.1 - 1 μm and form pores-pore size is about 0.1 - 1.0 μm. Meanwhile, in the form of pellets, porous HAp surface pores seem to have a bigger and more of HAp are not porous.