PENGAWETAN BAMBU TALANG SECARA SEDERHANA Eka Novriyanti; Edi Nurrohman 2)
Jurnal Penelitian Hasil Hutan Vol 22, No 4 (2004): Jurnal Penelitian Hasil Hutan
Publisher : Pusat Penelitian dan Pengembangan Hasil Hutan

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (2621.538 KB) | DOI: 10.20886/jphh.2004.22.4.223-230

Abstract

This research was conducted to examine the effectiveness of preserving bamboo with a Boron compound preservative. Four levels of concentrations, i.e 5,  10,  15,  and 20% were tested through simple method on bamboo talang (Schizostachyum brachycladum). Lower part of each culm was cut and debarked prior to one week soaking in the boric solution.  Results indicated that longitudinal penetration could reach 100%. Retention was varied in accord with boric concentration, but the 15%solution gave the highest retention. 
PENELAAHAN FAKTOR YANG DAPAT MEMPENGARUHI PENETAPAN UKURAN SASARAN VENIR KAYU LAPIS Eka Novriyanti
Jurnal Penelitian Hasil Hutan Vol 24, No 5 (2006): Jurnal Penelitian Hasil Hutan
Publisher : Pusat Penelitian dan Pengembangan Hasil Hutan

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.20886/jphh.2006.24.5.371-384

Abstract

Untuk mendapatkan konstruksi panel yang memiliki ukuran tebal yang diinginkan, maka diperlukan penetapan ukuran sasaran pada saat pengupasan venir.  Faktor-faktor penyusutan venir, pengempaan panel, pengampelasan, dan penyusutan panel serta keragaman pengupasan total dapat mempengaruhi penetapan ukuran sasaran. Data yang dikumpulkan dalam percobaan ini adalah adalah tebal venir sesudah kupas 1,76 mm, penyusutan venir 6,34%, pengaruh pengempaan 11,94%, pengaruh pengampelasan 0,44%, tebal venir dalam panel 1,22 mm, rata-rata tebal panel akhir 28,02 mm, dan penyusutan panel 1,42%.  Data-data tersebut selanjutnya diolah dengan formula yang diturunkan dari perubahan yang dialami venir sampai menjadi panel oleh proses produksi, untuk mendapatkan ukuran sasaran pengupasan venir kayu lapis konstruksi 19-lapis. Hasil perhitungan menunjukkan bahwa ukuran sasaran pengupasan venir adalah 1,870 ± 0,013 mm.
PENGAWETAN BAMBU TALANG SECARA SEDERHANA Eka Novriyanti; Edi Nurrohman 2)
Jurnal Penelitian Hasil Hutan Vol 22, No 4 (2004): Jurnal Penelitian Hasil Hutan
Publisher : Pusat Penelitian dan Pengembangan Hasil Hutan

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (2621.538 KB) | DOI: 10.20886/jphh.2004.22.4.223-230

Abstract

This research was conducted to examine the effectiveness of preserving bamboo with a Boron compound preservative. Four levels of concentrations, i.e 5,  10,  15,  and 20% were tested through simple method on bamboo talang (Schizostachyum brachycladum). Lower part of each culm was cut and debarked prior to one week soaking in the boric solution.  Results indicated that longitudinal penetration could reach 100%. Retention was varied in accord with boric concentration, but the 15%solution gave the highest retention. 
PENELAAHAN FAKTOR YANG DAPAT MEMPENGARUHI PENETAPAN UKURAN SASARAN VENIR KAYU LAPIS Eka Novriyanti
Jurnal Penelitian Hasil Hutan Vol 24, No 5 (2006): Jurnal Penelitian Hasil Hutan
Publisher : Pusat Penelitian dan Pengembangan Hasil Hutan

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.20886/jphh.2006.24.5.371-384

Abstract

Untuk mendapatkan konstruksi panel yang memiliki ukuran tebal yang diinginkan, maka diperlukan penetapan ukuran sasaran pada saat pengupasan venir.  Faktor-faktor penyusutan venir, pengempaan panel, pengampelasan, dan penyusutan panel serta keragaman pengupasan total dapat mempengaruhi penetapan ukuran sasaran. Data yang dikumpulkan dalam percobaan ini adalah adalah tebal venir sesudah kupas 1,76 mm, penyusutan venir 6,34%, pengaruh pengempaan 11,94%, pengaruh pengampelasan 0,44%, tebal venir dalam panel 1,22 mm, rata-rata tebal panel akhir 28,02 mm, dan penyusutan panel 1,42%.  Data-data tersebut selanjutnya diolah dengan formula yang diturunkan dari perubahan yang dialami venir sampai menjadi panel oleh proses produksi, untuk mendapatkan ukuran sasaran pengupasan venir kayu lapis konstruksi 19-lapis. Hasil perhitungan menunjukkan bahwa ukuran sasaran pengupasan venir adalah 1,870 ± 0,013 mm.