Journal of Health and Dental Sciences
Vol. 6 No. 2 (2026): Journal of Health and Dental Sciences

THE EFFECT OF ALKALI TREATMENT OF PINEAPPLE LEAF FIBER (Ananas comosus (L.) Merr.) BUNDLES ON THE IMPACT STRENGTH OF HEAT-POLYMERIZED ACRYLIC RESIN

Ainin Nafilatus Soumil Fitriyah (Department of Biomaterials and Dental Technology, Faculty of Dentistry, Institut Ilmu Kesehatan Bhakti Wiyata, Kediri, Indonesia)
Elok Nafilah Fitri (Department of Biomaterials and Dental Technology, Faculty of Dentistry, Institut Ilmu Kesehatan Bhakti Wiyata, Kediri, Indonesia)
Ida Wahyuningsih (Department of Dental Public Health and Preventive Dentistry, Faculty of Dentistry, Institut Ilmu Kesehatan Bhakti Wiyata, Kediri, Indonesia)



Article Info

Publish Date
01 Oct 2026

Abstract

Heat-polymerized acrylic resin is widely used as a denture base material but has low fracture resistance. Pineapple leaf fiber (PALF) is a natural reinforcement; however, its non-cellulosic components can hinder fiber–matrix adhesion. Alkali treatment removes lignin and hemicellulose, thereby improving interfacial bonding and mechanical properties. This study aimed to determine the effect of alkali-treated pineapple leaf fiber (Ananas comosus (L.) Merr.) bundles on the impact strength of heat-polymerized acrylic resin denture bases. A total of 24 acrylic resin specimens were divided into four groups (n = 6): a control group and three treatment groups treated with 3%, 5%, and 7% NaOH. The fibers were immersed in the respective NaOH solutions for 2 hours, bundled, and incorporated into the acrylic resin matrix. Impact strength was evaluated using an impact tester. The data were analyzed using one-way ANOVA followed by the LSD post hoc test, with a significance level of α = 0.05. The mean impact strength values were 4.80 ± 0.87 kJ/m² for Group I, 5.94 ± 0.77 kJ/m² for Group II, 7.69 ± 0.81 kJ/m² for Group III, and 5.08 ± 0.76 kJ/m² for Group IV. Alkali treatment with 3% and 5% NaOH increased the impact strength of heat-polymerized acrylic resin denture bases, whereas 7% NaOH reduced the impact strength. One-way ANOVA showed a significant difference among the treatment groups (p < 0.001), and the LSD post hoc test demonstrated that the 5% NaOH group differed significantly from the 3% and 7% NaOH groups. These findings indicate that alkali treatment with 5% NaOH resulted in the greatest increase in the impact strength of heat-polymerized acrylic resin compared with the other groups. DOI : 10.54052/jhds.v6n2.p187-200

Copyrights © 2026






Journal Info

Abbrev

jhds

Publisher

Subject

Dentistry

Description

Journal of Health and Dental Sciences or JHDS is a peer-reviewed and open access journal that focuses on promoting health and dental sciences generated from health and dental basic sciences, clinical, and community or public health and dental researches to integrate research in all aspects of human ...