THE EFFECT OF ALKALI TREATMENT OF PINEAPPLE LEAF FIBER (Ananas comosus (L.) Merr.) BUNDLES ON THE IMPACT STRENGTH OF HEAT-POLYMERIZED ACRYLIC RESIN Ainin Nafilatus Soumil Fitriyah; Elok Nafilah Fitri; Ida Wahyuningsih
Journal of Health and Dental Sciences Vol. 6 No. 2 (2026): Journal of Health and Dental Sciences
Publisher : Fakultas Kedokteran Gigi Unjani

Show Abstract | Download Original | Original Source | Check in Google Scholar

Abstract

Heat-polymerized acrylic resin is widely used as a denture base material but has low fracture resistance. Pineapple leaf fiber (PALF) is a natural reinforcement; however, its non-cellulosic components can hinder fiber–matrix adhesion. Alkali treatment removes lignin and hemicellulose, thereby improving interfacial bonding and mechanical properties. This study aimed to determine the effect of alkali-treated pineapple leaf fiber (Ananas comosus (L.) Merr.) bundles on the impact strength of heat-polymerized acrylic resin denture bases. A total of 24 acrylic resin specimens were divided into four groups (n = 6): a control group and three treatment groups treated with 3%, 5%, and 7% NaOH. The fibers were immersed in the respective NaOH solutions for 2 hours, bundled, and incorporated into the acrylic resin matrix. Impact strength was evaluated using an impact tester. The data were analyzed using one-way ANOVA followed by the LSD post hoc test, with a significance level of α = 0.05. The mean impact strength values were 4.80 ± 0.87 kJ/m² for Group I, 5.94 ± 0.77 kJ/m² for Group II, 7.69 ± 0.81 kJ/m² for Group III, and 5.08 ± 0.76 kJ/m² for Group IV. Alkali treatment with 3% and 5% NaOH increased the impact strength of heat-polymerized acrylic resin denture bases, whereas 7% NaOH reduced the impact strength. One-way ANOVA showed a significant difference among the treatment groups (p < 0.001), and the LSD post hoc test demonstrated that the 5% NaOH group differed significantly from the 3% and 7% NaOH groups. These findings indicate that alkali treatment with 5% NaOH resulted in the greatest increase in the impact strength of heat-polymerized acrylic resin compared with the other groups. DOI : 10.54052/jhds.v6n2.p187-200