Laterite steel with nickel content is expected to be a solution to overcome the lackof domestic steel availability and dependence on imports. This research was conducted to developNickel-Chromium-Molybdenum alloy steel used Grinding ball for cement industrial applications.Grinding ball is the one of imported steel products needed to be crushing and size reduction the oresor cement. In addition to import issues, grinding balls have a significant problem: their mechanicalproperties that do not meet SNI 1049 require the material to have a minimum hardness value of 45HRC. In this study, the characteristics of Nickel alloy steel were investigated further through heattreatment of forgings heated at the austenitizing temperature of 950 °C and austempering withvariations in the cooling medium of Sn/Zn solution. The cooling medium was chosen because it hasa melting temperature in the phase diagram area to form the bainite microstructure with complex andchallenging characteristics, both of which are required in material for grinding ball applications. Inparticular, the hardness value that passed the SNI 1069 standard was the use of samples with a CrMo alloy of 1%-wt with a hardness value of 45.92 HRC for Sn Austemper and 48.07 HRC for Znaustemper.
Copyrights © 2021