Abstract. The use of waste-derived materials in mortar offers an alternative approach to reduce conventional material consumption while improving waste utilization. This study investigated the setting characteristics and compressive strength of mortar incorporating sawdust, rice husk ash (RHA), and nickel slag. Sawdust and nickel slag were used as partial fine aggregate replacements, while RHA was used as a supplementary cementitious material. Six mixtures were prepared, consisting of one control mixture and five modified mixtures. RHA was maintained at 5%, while sawdust and nickel slag varied from 5% to 15%. Setting time was evaluated using Vicat tests, and compressive strength was measured on 50 mm cube specimens after 28 days of water curing. The use of 5% RHA increased the initial and final setting times from 105 to 120 min and from 180 to 200 min, respectively. The control mortar reached 21.10 MPa, while the modified mixtures achieved 18.00–21.80 MPa. Mixtures containing up to 10% sawdust maintained compressive strength comparable to the control. M4, containing 10% sawdust, 5% RHA, and 15% nickel slag, achieved 21.80 MPa, 3.32% above the control. The results indicate that balanced proportions of organic, pozzolanic, and mineral waste can maintain mortar mechanical performance. Keywords: sustainable mortar; sawdust; rice husk ash; nickel slag; compressive strength
Copyrights © 2026