PENGARUH PENAMBAHAN BUBUK ALUMINIUM DAN SILIKA FUME TERHADAP KUAT TEKAN DAN POROSITAS BETON NON PASIR Verby Reza Surya Nurdiana; Noviza Ramadhaningsih Aziz; Susi Hariyani; Innino Justitiannisa
NUSANTARA : Jurnal Ilmu Pengetahuan Sosial Vol 13, No 5 (2026): NUSANTARA : Jurnal Ilmu Pengetahuan Sosial
Publisher : Universitas Muhammadiyah Tapanuli Selatan

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.31604/jips.v13i5.2026.1006-1010

Abstract

Penelitian ini bertujuan untuk mengkaji pengaruh penambahan bubuk aluminium dan silica fume terhadap kuat tekan dan porositas beton non-pasir. Metode yang digunakan adalah eksperimen kuantitatif dengan variasi bubuk aluminium (0%, 0,3%, 0,5%, 0,7%, dan 0,9%) serta silica fume (0%, 2,5%, 5%, 7,5%, dan 10%) berdasarkan berat semen. Sampel paving block diuji pada umur 28 hari untuk mengetahui nilai kuat tekan dan porositas. Pengujian kuat tekan dilakukan menggunakan Compression Testing Machine (CTM), sedangkan porositas diukur dengan membandingkan volume rongga pada setiap benda uji. Hasil penelitian menunjukkan bahwa campuran optimum diperoleh pada penggunaan 0,9% bubuk aluminium dan 2,5% silica fume, dengan kuat tekan sebesar 42,55 kg/cm² dan porositas sebesar 21,07%. Penambahan bubuk aluminium cenderung meningkatkan porositas, sedangkan silica fume dapat meningkatkan kuat tekan. Penelitian ini memberikan kontribusi dalam pengembangan material paving block yang ramah lingkungan serta mampu mengurangi genangan air di permukaan pada area publik.
Analisis Substitusi Abu Ampas Tebu dan Garam terhadap Karakteristik Mekanis pada Stabilitas Tanah Laterit Bella Auliananingsih; Dila Ariyanti; Wattini Wattini; Innino Justitiannisa
Jurnal Talenta Sipil Vol 9, No 2 (2026): Agustus
Publisher : Universitas Batanghari Jambi

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.33087/talentasipil.v9i2.1428

Abstract

Soil stabilization is a technique commonly applied in construction projects to improve soil strength so that it can adequately support structural loads. In this study, lateritic soil was stabilized using additives in the form of sugarcane bagasse ash (SBA) and coarse salt. A quantitative research approach was employed through a series of laboratory tests. The mixture composition consisted of 3% SBA, while the coarse salt content was varied at 4%, 8%, 12%, 16%, and 20%. The California Bearing Ratio (CBR) test results for the natural soil showed values of 15.00% at 2.5 mm penetration and 19.11% at 5.0 mm penetration with 56 blows. After the addition of SBA and salt, the CBR values exhibited fluctuations. The highest CBR values were obtained from the mixture containing 3% SBA and 8% coarse salt with 56 blows, reaching 26.00% at 2.5 mm penetration and 30.22% at 5.0 mm penetration, indicating a significant improvement in soil bearing capacity. In contrast, the lowest CBR values were observed in the mixture of 3% SBA and 12% coarse salt with 25 blows, yielding only 2.40% at 2.5 mm penetration and 2.78% at 5.0 mm penetration, which indicates a substantial reduction in soil strength. The unconfined compressive strength (UCS) test results showed that the natural soil possessed the highest strength, with a maximum value of 5.88 kg/cm². After stabilization, the UCS values generally decreased, although the mixture with 8% salt still produced values close to those of the natural soil. However, increasing the salt content beyond 12% resulted in a significant decline in soil strength.
PENGARUH ABU AMPAS TEBU DAN LIATLIGBAL TERHADAP BETON MUTU TINGGI Indah Rosanti; Nurul Fitriani; Revo Nugraha Yudhandie; Raenaldhy Ardhyana Saputra; Innino Justitiannisa
Construction and Material Journal Vol. 8 No. 2 (2026): Construction and Material Journal Vol. 8 No. 2 Oktober 2026
Publisher : Politeknik Negeri Jakarta

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.32722/cmj.v8i2.8273

Abstract

High-strength concrete is defined in SNI 03-6468-2000 as concrete with a specified compressive strength of at least 41.4 MPa, whereas this study targeted a strength of 50 MPa. This experimental study evaluated the use of sugarcane bagasse ash and balloon-gas production waste (LIATLIGBAL) as a combined supplementary material in high-strength concrete. Four mixtures were prepared with combined additions of 0%, 6.5%, 9%, and 11% by cement mass. Twenty-four cylindrical specimens (150 mm × 300 mm) were cast and tested at curing ages of 14 and 28 days. Slump was measured once for each fresh-concrete batch and was not classified by curing age. The average slump values ranged from 8.1 to 10.3 cm. The 14-day compressive strengths of the normal, 6.5%, 9%, and 11% mixtures were 33.09, 35.84, 41.52, and 44.22 MPa, respectively. At 28 days, the corresponding strengths were 33.06, 39.26, 44.48, and 50.19 MPa. The 11% mixture achieved the highest compressive strength and met the 50 MPa research target. However, its water absorption was also the highest at 28 days, indicating that further durability evaluation is required. The results demonstrate the potential of sugarcane bagasse ash and LIATLIGBAL for high-strength concrete while supporting waste utilization in construction.