Green Corrosion Inhibition of Gas Pipelines Using Rice Husk Derived Nanocellulose and Plant Extract Inhibitors for Adsorption Chemistry and Flow Dynamics Nnadikwe Johnson; Samuel Kwelle; Okakpu Ogochukwu Judith; Amaefula Chibunma Vivian; Momoh Abdulazeez Adeyemi
Jurnal Teknik Indonesia Vol. 6 No. 01 (2027): Jurnal Teknik Indonesia (JU-TI), Inpres 2027
Publisher : SEAN Institute

Show Abstract | Download Original | Original Source | Check in Google Scholar

Abstract

The corrosion of mild steel in CO2-saturated 3.5% NaCl brine, representative of oil and gas pipeline environments, poses significant economic and safety challenges, necessitating the development of eco-friendly inhibitors. This study developed a green corrosion inhibitor based on rice husk-derived nanocellulose (CNC) functionalized with Azadirachta indica leaf extract (CNC-PE) and evaluated it on mild steel coupons under laboratory static and hydrodynamic conditions. CNC was extracted via alkaline treatment, bleaching and acid hydrolysis, yielding rod-like nanocrystals with average length of 180 ± 25 nm and crystallinity index of 82.4%. Phytochemical analysis revealed high phenolic content (68.4 mg GAE/g) and flavonoid content, with heteroatoms (N, O) acting as adsorption centres. Corrosion performance was evaluated using weight loss, potentiodynamic polarization (PDP) and electrochemical impedance spectroscopy (EIS) in CO2-saturated 3.5% NaCl at 30-70°C, inhibitor concentration of 200-1000 ppm, immersion time up to 72 h, and flow velocity of 0.5-2.5 m/s in a laboratory flow loop. In direct experimental tests, inhibition efficiency (IE%) increased with concentration and reached a maximum experimental value of 90.05% at 1000 ppm, with corrosion rate reduced from 3.82 mm/y (blank) to 0.38 mm/y under the same test conditions. PDP revealed mixed-type inhibition with cathodic predominance, while EIS showed charge transfer resistance increased from 42.5 to 425.8 Ω cm2. Adsorption obeyed the Langmuir isotherm with ΔG°ads of -33.8 kJ/mol, indicating mixed physisorption-chemisorption. Response Surface Methodology (RSM) with Central Composite Design (CCD) was then used for optimization. The model predicted an optimum IE% of 91.8% at 856 ppm, 34.2°C, 1.12 h and 0.6 m/s. This prediction was validated experimentally, giving an experimental IE% of 90.9% at the optimized conditions, corresponding to a 0.98% prediction error. This validated optimum (90.9%) is therefore distinct from the single-factor experimental maximum (90.05% at 1000 ppm). Flow loop tests showed the formulation maintained 81.5% IE at 2.0 m/s, compared to 68.0% for plant extract alone, indicating improved shear resistance under laboratory flow. The main contributions are: (1) valorization of rice husk agro-waste into functional CNC, (2) a clear experimental vs model distinction for IE%, and (3) evidence of a dense Fe-CNC-PE complex film blocking active sites under laboratory conditions. These findings support the potential of CNC-PE as a laboratory-scale green inhibitor candidate. Further field-scale, long-term, and high-pressure gas pipeline validation is required before industrial application.
Hydrogen-Natural Gas Blending in High-Pressure Subsea Transmission Pipelines: Mitigation of Embrittlement, Leakage and Flow Assurance Challenges Nnadikwe Johnson; Samuel Kwelle; Ifeanyi Lawrence Igbonekwu; Amaefula Chibunma Vivian; Momoh Abdulazeez Adeyemi
Jurnal Teknik Indonesia Vol. 6 No. 01 (2027): Jurnal Teknik Indonesia (JU-TI), Inpres 2027
Publisher : SEAN Institute

Show Abstract | Download Original | Original Source | Check in Google Scholar

Abstract

Repurposing existing subsea natural gas pipelines for hydrogen transport offers a cost-effective pathway for decarbonization, yet the integrity implications of hydrogen blending remain insufficiently understood. This study presents an integrated assessment of hydrogen embrittlement, leakage behavior and flow assurance for subsea pipelines carrying hydrogen-natural gas blends, based on systematic synthesis of 25 experimental and numerical studies complemented by analytical modelling. Hydrogen embrittlement assessment using Slow Strain Rate Test and fatigue crack growth data from the reviewed studies indicated that embrittlement index increased from 12.4% at 10% H2 to 41.3% at 30% H2 for X65 steel, and from 18.7% to 54.6% for X80 steel, suggesting higher susceptibility of higher-strength grades. Within the datasets reviewed, hydrogen partial pressure above 30 bar was associated with accelerated crack growth by up to 6.8 times, with heat-affected zones above 280 HV showing particular vulnerability. Leakage analysis based on a choked flow model indicated that for a 5 mm crack at 150 bar, mass leak rate decreased from 2.85 kg/s for pure natural gas to 2.41 kg/s at 20% H2, while volumetric rate increased by 18%. Subsea dispersion modelling indicated hydrogen bubbles rise 2.3 times faster and dissolve within 22-35 m, which may challenge surface detection. Flow assurance simulation using Peng-Robinson EOS, under the assumed pipeline geometry and operating conditions, indicated pressure drop increased from 18.2 bar to 28.4 bar across 100 km at 30% H2, requiring an estimated 12-15% additional compression power. Hydrate formation temperature decreased from 18.5°C to 14.8°C, offering partial benefit. An integrated risk framework suggests 20% H2 as a provisional screening threshold for X65 pipelines under the modelled conditions, corresponding to a modelled risk score of 5.2/10. This should not be interpreted as a safe operating limit or design recommendation. Internal coating combined with operational control reduced modelled risk by over 60% in the scenarios assessed.