Fajar Al Afghani
Unknown Affiliation

Published : 5 Documents Claim Missing Document
Claim Missing Document
Check
Articles

Found 5 Documents
Search

PENGARUH TEMPERATUR DAN KOMPOSISI Nb TERHADAP INTERDIFUSI PADUAN U-Zr-Nb Maman Kartaman Ajiriyanto; Masrukan Masrukan; Fajar Al Afghani; Yanlinastuti Yanlinastuti
Urania : Jurnal Ilmiah Daur Bahan Bakar Nuklir Vol 27, No 3 (2021): Oktober, 2021
Publisher : website

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/urania.2021.27.3.6503

Abstract

PENGARUH TEMPERATUR DAN KOMPOSISI Nb TERHADAP INTERDIFUSI PADUAN U-Zr-Nb. Telah dilakukan simulasi percobaan intermik bahan bakar U-Zr-Nb dengan pelat aluminium. Mula-mula dibuat ingot paduan U-6Zr-2Nb, U-6Zr-5Nb, dan U-6Zr-8Nb menggunakan tungku peleburan busur listrik. Ingot yang diperoleh dipotong-potong menjadi berukuran ketebalan 2-3 mm dan diameter sekitar 5-6 mm selanjutnya ditutup menggunakan pelat Al pada salah satu sisinya serta dipress. Setelah dipress, ingot paduan U-6Zr-2Nb, U-6Zr-5Nb, dan U-6Zr-8Nb   dipanaskan pada temperature 350 dan 450 °C selama 1 jam. Setelah dipanaskan ingot dikenai beberapa pengujian yaitu mikrostruktur menggunakan mikroskop optik dan Scanning Electron Microscope (SEM) yang dilengkapi dengan Energy Dispersive Spectrometer (EDS), kekerasan menggunakan uji kekerasan mikro, dan fasa dengan alat X-ray diffractometer (XRD). Hasil pemeriksaan mikrostruktur menunjukkan masih terlihat dengan jelas batas antara lapisan (interface) U-6Zr-2Nb, U-6Zr-5Nb, dan U-6Zr-8Nb dengan lapisan Al. Semakin tinggi kandungan Nb semakin rapat  rapat interface antara kedua lapisan.  Pada pengujian kekerasan mikro terlihat bahwa kekerasan pada interface sulit diukur sedangkan pada daerah U-Zr-Nb menunjukkan kenaikan kekerasan pada pemanasan dari 350 menjadi 450 °C, sedangkan pada bagian Al terjadi penurunan kekerasan pada kenaikan temperatur pemanasan dari 350 menjadi 450 °C.  Terbentuk senyawa UO3 pada semua sampel uji sedangkan fasa γ-U terbentuk pada sampel U-6Zr-2Nb baik yang dipanaskan pada temperatur 350 maupun 450 °C.Kata kunci:  Intermik, paduan U-Zr-Nb, aluminium, mikrostruktur, kekerasan, fasa.
PENGARUH PENAMBAHAN LARUTAN H3BO3 DAN LiOH TERHADAP PERILAKU KOROSI MATERIAL KELONGSONG ZIRCALOY-2 DALAM MEDIA AIR BEBAS MINERAL Fajar Al Afghani; Erwan Hermawan; Anditania Sari Dwi Putri; Ely Nurlaily
Urania: Jurnal Ilmiah Daur Bahan Bakar Nuklir Vol. 28 No. 1 (2022): Urania: Jurnal Ilmiah Daur Bahan Bakar Nuklir
Publisher : Badan Riset dan Inovasi Nasional

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/urania.2022.28.1.6609

Abstract

The primary coolant of the PHWR type reactor is controlled chemically by the addition of boric acid and LiOH to anticipate corrosion of the cladding material of Zr-2. This study aimed to analyze the effect of H3BO3 and LiOH solutions on the type and rate of of zircaloy-2 (Zr-2) corrosion in demineralized water. The corrosion test was carried out at room temperature to eliminate the influence of high temperature and pressure on the electrochemical process. In this study, the corrosion rate of Zr-2 was observed in a demineralized water solution with varying concentrations of H3BO3 and LiOH. The observation was done using Tafel method, where the addition of H3BO3 at concentrations of 10 ppm, 100 ppm, 500 ppm,1000 ppm and 2000 ppm resulted in corrosion rate of 17.29 x 10-3 mpy, 18. 51 x 10-3 mpy,20.82 x 10-3 mpy, 22.71 x 10-3 mpy and 23.29 x 10-3 mpy, respectively. The addition of 2000 ppm of H3BO3 and LiOH with varied concentrations of 1 ppm, 2 ppm, 3 ppm, 4 ppm results in decreasing of corrosion rate sequentially, namely 22.71 x 10-3 mpy, 21.88 x 10-3 mpy, 21.41 x 10-3 mpy, 21.39 x 10-3 mpy, whereas the addition of 5 ppm LiOH causes the corrosion rate to increase to 21.45 x 10-3 mpy. It can be concluded that the addition of LiOH and H3BO3 affects the corrosion rate of zircaloy-2 in demineralized water. Higher concentration of H3BO3 causes the corrosion rate to increase meanwhile, the addition of LiOH causes the corrosion rate to decrease to a concentration of 4 ppm. However, the addition of LiOH at a concentration of 5 ppm causes the corrosion rate to increase.
PENGARUH TEMPERATUR DAN KOMPOSISI Nb TERHADAP INTERDIFUSI PADUAN U-Zr-Nb Maman Kartaman Ajiriyanto; Masrukan; Fajar Al Afghani; Yanlinastuti Yanlinastuti
Urania: Jurnal Ilmiah Daur Bahan Bakar Nuklir Vol. 27 No. 3 (2021): Urania : Jurnal Ilmiah Daur Bahan Bakar Nuklir
Publisher : Badan Riset dan Inovasi Nasional

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/urania.2021.27.3.6503

Abstract

A simulation of U-Zr-Nb intermixed fuel has been carried out with aluminum plates. Initially, U-6Zr-2Nb, U-6Zr-5Nb, and U-6Zr-8Nb alloy ingots were made using an electric arc melting furnace. The ingot obtained was cut into pieces with a thickness of 2-3 mm and a diameter of about 5-6 mm, then it was covered Al plate on one side and pressed. After pressing, the alloy ingots of U-6Zr-2Nb, U-6Zr-5Nb, and U-6Zr-8Nb were heated at temperatures of 350 and 450 oC for 1 hour. The ingot was subjected to several tests, namely microstructure examination using optical microscope and Scanning Electron Microscope (SEM) equipped with Energy Dispersive Spectrometer (EDS), hardness test using microhardness tester, and phase observation using X-ray diffractometer (XRD). The results of microstructure examination show that the boundaries between the U-6Zr-2Nb, U-6Zr-5Nb, and U-6Zr-8Nb layers (interfaces) and the Al layer were clearly visible. The higher of the Nb content, the denser the interface between the two layers. For the microhardness test, we found that the hardness at the interface was difficult to measure, while the U-Zr-Nb region shows an increase in hardness for heating from 350 to 450 oC, while in the Al section there is a decrease in hardness when the heating temperature increases from 350 to 450 oC. UO3 compounds were formed in all test samples while the γ-U phase was formed in U-6Zr-2Nb samples both heated at temperatures of 350 and 450 oC.
PENGARUH HIDROGEN TERHADAP KEKUATAN TARIK KELONGSONG BAHAN BAKAR NUKLIR BERBASIS PADUAN ZIRKONIUM Rohmad Sigit; Fajar Al Afghani; Jan Setiawan; Sungkono
Urania: Jurnal Ilmiah Daur Bahan Bakar Nuklir Vol. 23 No. 3 (2017): Urania : Jurnal Ilmiah Daur Bahan Bakar Nuklir
Publisher : Badan Riset dan Inovasi Nasional

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.17146/urania.2017.23.3.3648

Abstract

During reactor operation, zircaloy-4 (Zr-4) as fuel cladding is under an environment that can potentially cause mechanical failure, especially by the effect of cladding-hydrogen interaction. Hydrogen would diffuse and precipitate to form brittle hydrides when the solubility limit is surpassed. In this experiment, ring tensile test method was used to examine the effect of hydrides existence on tensile strength of Zr-4 cladding. The Zr-4 sample was annealed at 500 °C and 600 °C for an hour in vacuum condition and followed by hydriding with a pressure up to 1000 mbar with 3 hours holding time and slow cooling. According to ideal gas equation, hydrogen content in Zr-4 reaches about 674 ppm and 1215 ppm at hydriding temperature of 500 °C and 600 °C respectively. Microstructure observation shows that hydrides precipitate was formed at grain boundaries. The hydrides were found to be longer and thicker at higher hydriding temperature. As the hydrogen content increases, the ring tensile test shows increasing stress at 4.4 %, decreasing strain at 2.1 % and increasing microhardness level at 13 %. This result confirms that the existence of hydrides precipitates in cladding has an effect of increasing the tensile strength and decreasing the ductility obviously.
MODEL SIMULATION OF THE EFFECT OF ZINC PHOSPHATE INHIBITOR ON CORROSION RATE OF SECONDARY COOLING PIPE FOR PRESSURIZED WATER REACTOR USING PREDICTOR-CORRECTOR METHOD Fajar Al Afghani; Maman Kartaman Ajiriyanto; Rosika Kriswarini; Arif Nugroho; Juan Carlos Sihotang; Ely Nurlaily; Anditania Sari Dwi Putri
Urania: Jurnal Ilmiah Daur Bahan Bakar Nuklir Vol. 30 No. 1 (2024): Urania: Jurnal Ilmiah Daur Bahan Bakar Nuklir
Publisher : Badan Riset dan Inovasi Nasional

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.55981/Urania.2024.8677

Abstract

Corrosion is one of the unavoidable problems in nuclear reactor cooling systems. Secondary Cooling Pipe Multi-Purpose Reactor G.A Siwabessy (MPR-GAS) based on low carbon steel is very easy to oxidize because it is an open circulation cooling system. Zinc-phosphate inhibitor (ZnPO4) is one of the inhibitors used to inhibit the corrosion reaction that occurs between the low carbon steel cooling pipe and the cooling water environment. The research has been carried out on numerical calculations to find a solution for the corrosion rate model of steel with and without an inhibitor by the Predictor-corrector method. The simulation results show that the effect of ZnPO4 inhibitor on the corrosion rate of steel is seen as a relationship between inhibitor concentration and stable time, if the inhibitor concentration increases, the stable time will also increase. The rate of corrosion that occurs (reducing the concentration of corroded product). Therefore, the recommended inhibitor concentration value is 0.9% for models in 0.1 M HCL medium. This concentration is the most appropriate concentration to slow down the corrosion rate most minimal.