Bioplastics have emerged as a sustainable alternative to conventional petroleum-based plastics. This study investigates the effect of nanochitosan–catechin ratio and glycerol concentration on the properties of polylactic acid (PLA)/polycaprolactone (PCL)-based bioplastics. Nanochitosan was utilized as a reinforcing agent, while catechin derived from jamblang seeds served as a bioactive compound. Bioplastics were fabricated via melt blending with varying nanochitosan ratios (0.3:0.7–0.7:0.3) and glycerol concentrations (0–4%). The resulting materials were characterized using tensile testing, Fourier Transform Infrared (FTIR) spectroscopy, Thermogravimetric Analysis (TGA), and biodegradation testing. The results indicated that the highest tensile strength (31.3 MPa) was achieved at a nanochitosan ratio of 0.6:0.4 with 1% glycerol. FTIR analysis confirmed the presence of O–H, N–H, C–H, C=O, and C–O functional groups without the formation of new bonds, indicating physical interactions through hydrogen bonding. TGA results revealed good thermal stability with an onset temperature of 359.74°C. Furthermore, biodegradation analysis showed a mass loss of 13.54% after 18 days. These findings demonstrate that the incorporation of nanochitosan, catechin, and glycerol significantly influences the mechanical, thermal, and biodegradation properties of PLA/PCL-based bioplastics.Keywords : Polylactid Acid (PLA), Polycaprolactone (PCL), Nanochitosan, Catechin, glycerol
Copyrights © 2026