Analysis of SrTiO3 ceramics with the doping Cuprum(II) acetate (Cu(CH3COO)2), the variation in the concentration of doping used 0%; 0,5%; and 1% using the solid state reaction method was successful. The annealing process is carried out starting from room temperature then raised to an annealing temperature of 850 oC with a temperature increase of 1,67 oC / minute and held constant for 8 hours. Next proceed with the cooling process until it returns to room temperature for 13 hours. Analysis of XRD data using the Cramer-Cohen method yielded a lattice parameter of 3,909 Å; 3,906 Å; and 3,905 Å, a cubic crystal structure.