The results showed the use of cow dung waste can increase the compressive strength of hollow brick from any composition of waste. Hollow brick with cow dung substitution of 0% has an average compressive strength value 44.75 Kg/Cm2 has an average water absorption of 14.31%, hollow brick with cow dung substitution of 5% has a value of compressive strength average 47.47 Kg/Cm2 has an average water absorption of 15.67%, Batako perforation with cow dung substitution of 7.5% has an average compressive strength value of 51.83 Kg/Cm2 has the absorption water averaging 13.71%, batako perforated with substitution of cow dung waste of 10% has an average compressive strength value 53.81 Kg/Cm2 has an average water absorption of 10.04%, hollow brick with substitution cow dung waste of 12.5% has an average compressive strength value of 50.66 Kg/Cm2 has an average water absorption of 23.6%, hollow brick with cow dung substitution of 15% average 48.84 Kg/Cm2 has an average water absorption of 19.72%. The optimum compressive strength value was obtained from percentage substitution of cow dung waste at 10% with mean value of compressive strength 53,81 Kg/Cm2 with average water absorption 10,04%.
Copyrights © 2020