Eggshell waste is a potential sustainable resource for cement-based materials; however, the effects of nano-eggshell powder (NESP) addition under different curing environments require further clarification. This study investigated mortar containing NESP at 5% and 10% as an additional material under freshwater and seawater curing. Six variations were evaluated through compressive strength at 7, 28, and 91 days, and water absorption, porosity, and electrical resistivity at 28 and 91 days. The results showed that NESP addition produced different responses depending on dosage, curing environment, and testing age. Under freshwater curing, the control mortar reached 25.89 MPa at 91 days, whereas seawater curing produced a maximum strength of 26.90 MPa at 28 days before declining at 91 days. Nevertheless, the NESP-free control exhibited the highest compressive strength at every testing age under both curing media, showing that NESP addition did not enhance strength. NESP-added variations generally exhibited higher water absorption and porosity, with ESXA-TS reaching 12.10% absorption and 22.10% porosity at 91 days. Electrical resistivity exceeded 100 kΩ·cm for all variations, although its development differed from the physical transport properties. Regression analysis showed that compressive strength was strongly and inversely related to porosity (R² = 0.94), whereas resistivity was practically unrelated to porosity, water absorption, or strength (R² ≤ 0.03). Therefore, NESP addition did not consistently improve mortar performance, and its effect depended on dosage, curing medium, and age.
Copyrights © 2026