cover
Contact Name
-
Contact Email
-
Phone
-
Journal Mail Official
-
Editorial Address
-
Location
Kota adm. jakarta selatan,
Dki jakarta
INDONESIA
JURNAL SELULOSA
ISSN : -     EISSN : -     DOI : -
Core Subject : Education,
Jurnal Selulosa (JSel) is a journal that provides scientific information resources aimed at researchers and engineers in academia, research institutions, government agencies, and industries. Jurnal Selulosa publishes original research papers, review articles and case studies focused on cellulose, cellulose derivatives, pulp technology, paper technology, environment, biorefinery and other related topics. Formerly known as Berita Selulosa, and the first publication was in 1965. Since 2011, the journal renamed to Jurnal Selulosa.
Arjuna Subject : -
Articles 7 Documents
Search results for , issue "Vol 42, No 02 (2007): BERITA SELULOSA" : 7 Documents clear
PENINGKATAN KUALITAS SERAT SEKUNDER DENGAN PERLAKUAN ENZIM DAN POLIMER Tri Wahyudi Widiastono; Hawasul Zein Muflihin
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (199.547 KB) | DOI: 10.25269/jsel.v42i2.193

Abstract

Research on enhancement of deinked pulp (DIP) freeness, is conducted by using cellulase along with polyacrylamide. The cellulase dosage varies at 0 - 0.3 %, and polyacrylamide 0 - 0.1%, based  on bone dry pulp weight. Reaction time is set at 30 minutes with the temperature at 50 °C. The result showed that the improvement freeness accompanied by the improvement of tensile strength, tear resistance, and porosity, but bursting strength and whiteness slightly decrease. Optimum improvements of paper quality due to enhancement of DIP, are reached by using 0.2% cellulose and 0.05% polyacrylamide., INTISARI Penelitian ini dilakukan pada stok deinked pulp (DI) untuk meningkatkan derajat giling dengan menggunakan selulase yang dipadukan dengan poliakrilamida. Dosis selulase divariasikan pada 0-0,3% dan poliakrilamida 0-0,1%, per berat kering pulp. Sedangkan waktu reaksi ditentukan 30 menit dengan suhu reaksi 50°C. Hasil penelitian menunjukkan kenaikan derajat giling disertai dengan peningkatan sifat ketahanan tarik, sobek, dan porositas. Sementara ketahanan retak dan derajat putih mengalami sedikit penurunan. Pada penggunaan selulase 0,2% dan poliakrilamida 0,05% kinerja DIP meningkat sedemikian sehingga  kualitas kertas optimal.
POTENSI DAN PENGARUH TANAMAN PADA PENGOLAHAN AIR LIMBAH PULP DAN KERTAS DENGAN SISTEM LAHAN BASAH Sri Purwati; Aep Surachman
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (206.118 KB) | DOI: 10.25269/jsel.v42i2.187

Abstract

Research on the pulp and paper effluents treatment by the wetland system process using mendong plant was conducted. Experiment was carried out in a laboratory scale to study the influence of plant on the treatment efficiency of waste water. The potency of plant in the wetland system was also studied both the effects on the land quality and the plant yields. The experiment results showed that treatment by the wetland system process using mendong plant can increase the efficiency of pollutant removal in the waste water. At the retention time of 30 hours and the organic loading rate of 0.5 gr COD/m3, day, the treatment system could increase removal of COD 11 – 13 %, BOD 15 -16%, Lignin 3 – 4% and Na 20-33%. The treatment system, can also improve land quality, increase vegetative growth and productivity of the plant. Finally, based on heavy metal analysis, it  shows that mendong plant (Fimbristylis globulosa) is able to absorb heavy metal, especially Chromium (Cr) and Cadmiun (Cd) at 39-50% efficiency.ABSTRAKPenelitian pengolahan airlimbah pulp dan kertas dengan proses sistem lahan basah yang menggunakan tanaman mendong (Fimbristylis globulosa) telah dilakukan dalam skala laboratorium. Pengaruh dan potensi tanaman telah dipelajari melalui pengamatan efisiensi pengolahan air limbah dan juga efeknya terhadap kualitas tanah serta pertumbuhan tanaman. Hasil percobaan menunjukkan bahwa dengan menggunakan tanaman dalam sistem lahan basah dapat meningkatkan efisiensi reduksi kandungan pencemar dalam air limbah. Pada laju beban organic 0,5 gr COD/m3, hari, dengan waktu tinggal 30 jam dapat meningkatkan reduksi COD 11 – 13%, BOD 15-16%, lignin 3- 4% dan natrium 20-30%. Keunggulan pengolahan air limbah dengan sistem ini adalah kualitas tanah jadi meningkat sehingga meningkatkan produktivitas tanaman yang tumbuh pada tanah tersebut. Selain itu diperoleh hasil bahwa tanaman mendong mempunyai kemampuan menyerap logam berat khususnya Chromiun (Cr) dan Cadmium (Cd) yang terkandung dalam air limbah dengan efisiensi reduksi 39 – 50%
Sari Pustaka Hendro Risdianto
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (165.499 KB) | DOI: 10.25269/jsel.v42i2.194

Abstract

.
PENYISIHAN SENYAWA KLOROLIGNIN OLEH Phanerochaete chrysosporium DALAM BIOREAKTOR UNGGUN TERFLUIDISASI Dwina Roosmini; Wisjnuprapto Wisjnuprapto; Reski Dian Diniari; Junianti Roslinda
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (227.55 KB) | DOI: 10.25269/jsel.v42i2.188

Abstract

Chlorolignin compound in pulp and paper wastewater are toxic and mutagenic. The pulp and paper wastewater consisting chlorolignin are harmful if discharged to the receiving water without treatment. Biological treatment is an alternative to treat the chlorolignin. White rot fungi Phanerochaete chrysosporium with extra cellular enzyme are able to degrade chlorolignin. This study is conducted by using fluidized bed reactor to treat chlorolignin by using immobilized Phanerochaete chrysosporium. This study are intended to find the ability of  Phanerochaete chrysosporium in degrading chlorolignin in the range of concentration (0.05g/L; 0.1g/L; 0.2g/L; 0.3 g/L and 0.4 g/L). The molecular distribution of chlorolignin before and after treatment is measured by using High Performance Liquid Chromatography. This study showed that Phanerochaete chrysosporium are able to depolymerization high molecular chlorolignin to low molecular. INTISARISenyawa klorolignin, yang terdapat pada air buangan industri pulp dan kertas, merupakan senyawa lignin yang terklorinasi. Senyawa ini bersifat toksik dan mutagenik dan akan sangat berbahaya bila langsung dibuang ke perairan tanpa mengalami pengolahan terlebih dahulu. Pengolahan secara biologis merupakan alternatif yang tepat untuk mengolah klorolignin. Jamur Phanerochaete chrysosporium diketahui memiliki enzim ekstraseluler yang mampu mendegradasi senyawa aromatik tersebut. Pada penelitian ini digunakan bioreaktor unggun terfluidisasi sebagai tempat terjadinya reaksi. Pada penelitian dilakukan variasi konsentrasi klorolignin 0,05 g/L; 0,1 g/L; 0,2 g/L; 0,3 g/L; dan 0,4 g/L. Konsentrasi glukosa yang dipakai ialah konsentrasi dimana efisiensi penyisihan optimum, yaitu penyisihan lignin 62,02% dan warna 75,05%. Perubahan distribusi berat molekul klorolignin sebelum dan sesudah pengolahan diperiksa dengan menggunakan metoda kromatografi cair kinerja tinggi. Hasil yang diperoleh menunjukkan bahwa jamur Phanerochaete chrysosporium mampu melakukan depolimerisasi senyawa klorolignin berat molekul tinggi menjadi senyawa-senyawa dengan berat molekul yang lebih rendah.
PENANGGULANGAN STICKIES KERTAS BEKAS MENGGUNAKAN BENTONIT DAN TALK Jenni Rismijana
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (188.02 KB) | DOI: 10.25269/jsel.v42i2.189

Abstract

The flotation deinking of ONP and OMG mixture has been done in the laboratory. ONP and OMG was repulped  separately at 4% consistency using NaOH, Na2SiO3 and H2O2 , up to 350 ml CSF. The mixture of 30% ONP and 70% OMG was made, then 1% dispersant, 0,5% collector, and 0 – 2% bentonite and  or talk were added to the mixture. Flotation was conducted for 15 minutes at 20 litre/minute air flow rate and 1500 rpm agitations to produce deinked pulp. Deinked pulp then converted to 80 gsm hand sheet. The hand sheets were tested for  the physical and  optical properties along with stickies and dirt. The results showed that the using of bentonite and talk, decrease the  stickies and dirt content as well as opacity, but increase the brightness. The usage of 2 % of bentonite decreases 93,8% of stickies and 84,1% of dirt, and for 2% talk the stickies and dirt decrease 92,9% and 83,1% respectively. Bentonite and talk also increase the strength of the handsheets and reached the maximum at 1,5% bentonite and 1% talk. INTISARI            Percobaan deinking campuran koran bekas  dan majalah bekas  secara flotasi telah dilakukan pada skala laboratorium. Koran bekas dan majalah bekas secara terpisah mengalami penguraian pada konsistensi 4% dengan penambahan NaOH, Na2SiO3 dan H2O2 sampai dicapai derajat giling sekitar 350 ml CSF. Kemudian dicampur dengan komposisi 30% koran dan 70% majalah. Pada stok campuran ditambahkan dispersan 1% dan kolektor 0,5%, kemudian bentonit dan atau talk masing-masing ditambahan dengan variasi 0 – 2%. Selanjutnya dilakukan proses flotasi selama 15 menit dengan laju alir udara 20 liter/menit dan agitasi 1500 rpm. Deinked pulp hasil flotasi kemudian dibuat lembaran dengan gramatur 80 g/m2. Terhadap lembaran yang dihasilkan, dilakukan pengujian sifat fisik, optik, luas stickies dan jumlah noda. Hasil percobaan menunjukkan penambahan bentonit dan talk dapat menurunkan luas stickies dan noda pada lembaran serta meningkatkan derajat putih tetapi menurunkan opasitas. Penambahan bentonit sebesar 2% menurunkan luas stickies sebesar 93,8% dan noda 84,1%, sedangkan penambahan talk 2% menurunkan luas stickies 92,9% dan noda 83,1%. Penambahan bentonit dan talk juga meningkatkan nilai indeks kekuatan dimana peningkatan tertinggi dicapai pada penambahan bentonit 1,5%.
PEMANFAATAN CAMPURAN LIMBAH PADAT DENGAN LINDI HITAM DARI INDUSTRI PULP DAN KERTAS SEBAGAI BAHAN BIOBRIKET Syamsudin Syamsudin; Sri Purwati; Ike Rostika
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (183.414 KB) | DOI: 10.25269/jsel.v42i2.191

Abstract

Utilization of solid waste and black liquor mixture from pulp and paper mills has been investigated. Sludge A comes from pulp and paper mill with non wood raw materials has heat value 2712 cal/g and ash content 29.8%; Sludge B from paper mill with wastepaper raw material and deinking process has heat value 2331 cal/g and ash content 25.9%; black liquors from pulp mill with soda process has 5579 cal/g and ash content 12.1%. The sludges which has already ground and homogeneous was mixed with strong black liquors and densified to form biobriquette. At the composition 0 – 40 % of black liquor, heat value increase to 3711 and 3513 cal/g for sludge A and B respectively.Black liquor can increase burning efficiency due to the decreasing of  ash content, but increasing heavy metal contents such as Pb, Cd, Cr, and Na. At the composition 30 – 40 % of black liquor, the pressing force biobriquette increase from 19 - 26 kg to 50 - 54 kg. This  means that the pressing force of biobriquette greater than coal (37 kg).INTISARIPemanfaatan campuran limbah padat indusri pulp dan kertas dengan lindi hitam sebagai bahan biobriket telah diteliti. Lumpur A berasal dari pabrik pulp dan kertas terpadu dengan bahan baku non kayu mempunyai nilai panas 2712 kal/g dan kadar abu 29,8%; lumpur B dari pabrik kertas dengan bahan baku kertas bekas dan proses deinking mempunyai nilai panas 2331 kal/g dan kadar abu 25,9%; dan lindi hitam dari larutan pekat sisa pemasakan pulp proses soda mempunyai nilai panas 5579 kal/g dan kadar abu 12,1%. Lumpur yang sudah halus dan homogen dicampur dengan lindi hitam pekat dan dicetak menjadi biobriket. Pada variasi lindi hitam 0 – 40% nilai panas meningkat menjadi 3711 dan 3513 kal/g, masing-masing untuk lumpur A dan lumpur B. Penambahan lindi hitam menurunkan kadar abu sehingga memberi pengaruh positif terhadap efisiensi pembakaran tetapi menaikkan kandungan logam berat Pb, Cd, Cr, dan Na. Pada penambahan lindi hitam 30 – 40% kuat tekan biobriket meningkat dari 19 – 26 kg menjadi 50 – 54 kg. Hal ini berarti kuat tekan biobriket lebih besar dibandingkan dengan batu bara yang memiliki kuat tekan 37 kg. 
TINGKAT TOKSISITAS PENTAKLOROFENOL TERHADAP ORGANISME AIR TAWAR Soetopo, Rina Susilowati; Wardana, Krisna Adhitya; Indrasari, Ilisya P.
JURNAL SELULOSA Vol 42, No 02 (2007): BERITA SELULOSA
Publisher : Center for Pulp and Paper

Show Abstract | Download Original | Original Source | Check in Google Scholar | Full PDF (270.347 KB) | DOI: 10.25269/jsel.v42i2.192

Abstract

Pentachlorophenol is one of the AOX compound components found in pulp bleaching effluents. Pentachlorophenol is bioaccumulative with the  bioconcentration factor in  Daphnia magna about 400 ( OSPARCOM, 1999). The research on the influence of pentachlorophenol to aquatic organism Daphnia magna have been conducted at neutral pH and temperature 29oC. It was carried out in 2 stages that are acute toxicity test for 24 hour and chronic toxicity test for one cycle live based on OECD guidelines 202 (1984). Acute toxicity test carried out at a range pentachlorophenol concentration about 300 - 550 ppb. Chronic toxicity test conducted with the semi-static  method at three pentachlorophenol concentration namely 0,16 pp,; 1,6 ppb, and 16 ppb. Data of  acute toxicity test  are analyzed by probit analysis to calculate the 24 hour EC50 immobilization concentration (EC50-24h) with 95% confidence limit. Data from chronic toxicity test are calculated to find out daily survivorship, daily age specific fecundity, and net reproductive rate according to Sorensen ( 1996). The results of experiments indicate that pentachlorophenol have the EC50-24 hour value to Daphnia Magna at about 359 – 455 ppb. The chronic effect of pentachlorophenol to Daphnia magna are decreasing mean daily survivorship, mean daily age specific fecundity, and mean net reproductive rate. INTISARI Pentachlorophenol adalah salah satu komponen senyawa AOX yang terdapat dalam air limbah proses pemutihan pulp. Pentaklorofenol bersifat bioakumulatif dengan faktor biokonsentrasi dalam organisme Daphnia magna 400 (OSPARCOM, 1999). Percobaan pengaruh pentaklorofenol terhadap organisme perairan Daphnia magna telah dilakukan pada pH netral dan suhu sekitar 29oC. Percobaan dilakukan dalam 2 tahap yaitu uji toksisitas akut dilakukan selama 24 jam dan uji toksisitas kronis dilakukan selama satu siklus hidup mengacu pada metoda OECD 202 (1984). Uji toksisitas akut dilakukan pada 5 konsentrasi pentaklorofenol (300 – 550 ppb). Uji toksisitas kronis dilakukan dengan metoda semi statis pada 3 konsentrasi pentaklorofenol yaitu  0,16 ppb, 1,6 ppb dan 16 ppb. Terhadap data uji toksisitas akut dilakukan perhitungan nilai EC50 dengan analisa probit, dan terhadap data uji toksisitas kronis dilakukan perhitungan kesintasan harian (survivorship, Ix), fekunditas harian (age spesific fecundity, mx), dan laju reproduktif bersih (net reproductive rate, Ro) menurut Sorensen (1996). Hasil percobaan, menunjukkan bahwa pentaklorofenol memiliki nilai EC50-24jam terhadap organisme akuatik Daphnia magna berkisar antara 359 – 455 ppb dan bersifat  kronis. Efek kronis pentaklorofenol terhadap Daphnia magna adalah menurunkan kesintasan harian, fekunditas harian, dan laju reproduktif bersih.