cover
Contact Name
A. Jannifar
Contact Email
polimesin@pnl.ac.id
Phone
+628126930456
Journal Mail Official
polimesin@pnl.ac.id
Editorial Address
Politeknik Negeri Lhokseumawe Jl. Banda Aceh-Medan Km 280 Buketrata, Lhokseumawe, 24301, Aceh, Indonesia
Location
Kota lhokseumawe,
Aceh
INDONESIA
Jurnal Polimesin
ISSN : 16935462     EISSN : 25491199     DOI : http://dx.doi.org/10.30811/jpl
Polimesin mostly publishes studies in the core areas of mechanical engineering, such as energy conversion, machine and mechanism design, and manufacturing technology. As science and technology develop rapidly in combination with other disciplines such as electrical, Polimesin also adapts to new facts by accepting manuscripts in mechatronics. In Biomechanics, Mechanical study in musculoskeletal and bio-tissue has been widely recognized to help better life quality for disabled people and physical rehabilitation work. Such a wide range of Polimesin could be published, but it still has criteria to apply mechanical systems and principles. Exceeding the limitation has been a common reason for rejection by those outside the scope. Using chemical principles more than mechanical ones in material engineering has been a common reason for rejection after submission. Excessive exploration of the management within the discipline of Industrial Engineering in the manufacturing technology scope is also unacceptable. The sub-scope biomechanics that focuses on ergonomics and does not study movement involving applied force on the bio-tissue is also not suitable for submission.
Articles 664 Documents
Comparative catalytic pyrolysis of polypropylene waste using natural zeolite and dolomite: effect of temperature on syn-oil yield and fuel properties Harmen Harmen; Hadi Prayitno; Amrul Amrul; Hendi Hidayat; Yoga Kurnia; Indra Mamad Gandidi
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9145

Abstract

Polypropylene (PP) waste accumulation requires effective thermochemical valorization via catalytic pyrolysis to recover synthetic oil (syn-oil). This study compared the performance of inexpensive natural zeolite and dolomite catalysts under identical fixed-bed reactor conditions. Pyrolysis runs were executed using 1,600 g of post-consumer PP waste (0.5-2 cm) heated via an LPG burner at 400 °C, 450 °C, and 500 °C. Product yields, operational metrics, and syn-oil fuel properties were systematically evaluated. The highest syn-oil yield reached 79.3% using 7% zeolite loading at 400 °C, while the dolomite series achieved its peak yield of 76.9% at 15% loading at 450 °C. Zeolite-derived syn-oil exhibited the maximum energetic properties, producing a calorific value of 45.9 MJ/kg and an octane rating of 78.2 RON. Conversely, increasing the operating temperature to 500 °C accelerated hydrocarbon cracking, which minimized processing time to 30 minutes and minimized external LPG fuel consumption, though it reduced liquid volume recovery due to enhanced gas formation. Factually, natural zeolite at 400 °C is the optimum condition to maximize liquid fuel volume, whereas 15% dolomite at 450 °C offers a viable alternative for decentralized operations. Due to the exploratory nature of the single-observation matrix, replicate experiments and engine testing are recommended before industrial scale-up.
Injection molding process optimization for PMMA lens manufacturing through machine tonnage migration: a comparative industrial study Dodi Mulyadi; Amir Amir; Rizki Aulia Nanda; Karyadi Karyadi; Agus Supriyanto; Nana Rahdiana; Ade Suhara
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9941

Abstract

The manufacturing of optical automotive lamp lenses using polymethyl methacrylate (PMMA) requires precise control of injection molding parameters to ensure consistent visual quality and production efficiency. This study investigates the optimization of injection molding process parameters for an automotive headlamp lens (PMMA Clear Sumipex MH011, two-cavity mold) through machine migration from a 450-ton injection molding machine to a Toshiba EC650SX III 650-ton machine. Under the initial production conditions, the limited screw drive capacity of the 450-ton machine resulted in excessive charging torque, requiring barrel temperatures up to 291°C to maintain stable plastication. Process optimization included runner system modification, barrel temperature reconfiguration, and multistage injection speed optimization. Production performance was evaluated using actual industrial data collected over a continuous 24-hour production period. The optimized process reduced runner weight by 27% (53.66 g to 39.20 g), shortened fill time from 7.61 s to 4.88 s, and decreased the actual cycle time from 69.0 s to 61.9 s, corresponding to an increase in theoretical production rate from approximately 52 to 58 shots/h. Actual 24-hour gross production increased from 2,406 to 2,496 pieces. Product yield also improved from 88.23% to 93.72%, while silver streak defects were reduced from 153 to 26 occurrences (83% reduction). A negative binomial regression analysis showed a significant association between machine/process configuration and silver streak occurrence (IRR = 5.89, p 0.001). The results indicate that combining higher machine capacity with optimized processing parameters improves production efficiency, process stability, and visual quality performance in industrial PMMA injection molding.
DSC-based thermal characterisation of recycled polycarbonate subjected to repeated reprocessing Cahyo Budiyantoro; Didik Puji Mulyanto
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.8915

Abstract

Polycarbonate (PC) is widely used in engineering applications because of its excellent mechanical properties, dimensional stability, and thermal resistance. However, repeated thermal processing during mechanical recycling may alter its thermal behavior, while quantitative information regarding thermal-response changes after multiple reprocessing cycles remains limited. This study aimed to investigate the effect of repeated reprocessing cycles on the thermal response of recycled polycarbonate using Differential Scanning Calorimetry (DSC). The contribution of this study is the systematic evaluation of how DSC-observed thermal responses evolved across 3, 6, and 9 controlled reprocessing cycles, enabling relatively small early-cycle changes to be distinguished from the more pronounced shifts observed at higher reprocessing histories. Virgin PC and recycled PC samples were prepared through repeated remelting and reprocessing. Thermal characterization was performed using DSC according to ASTM D3418 and ISO 11357-2. The glass transition temperature (Tg) and DSC-observed degradation-related thermal event temperature (Td) were evaluated to assess changes in thermal response associated with repeated reprocessing. The results showed that Tg gradually decreased from 149.47 °C for virgin PC to 148.53 °C, 146.79 °C, and 145.17 °C after 3, 6, and 9 cycles, respectively. Td initially increased slightly from 451.59 °C to 455.33 °C after 3 cycles, then decreased to 435.13 °C and 429.29 °C after 6 and 9 cycles. Overall, repeated reprocessing was associated with gradual shifts in thermal response, reflected by changes in Tg and DSC-observed degradation-related thermal events.
Microstructure and crystallinity characterization of graphite from petroleum coke for generation IV nuclear reactor material applications Syaiful Arif; Gunawarman Gunawarman; Syaiful Bakhri; Deni Mustika; Kusnanto Kusnanto; Maman Kartaman Ajiriyanto
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9130

Abstract

This study aims to analyze the effect of particle size on the microstructural evolution and chemical transformation of petroleum coke as a graphite material precursor for Generation IV nuclear reactor applications. Samples were prepared in two size variations, namely 5 mm and 100 mm, then subjected to thermal treatment at a temperature of 800 °C with a heating rate of 5 °C/min and a holding time of 2 hours in confined atmospheric conditions. Characterization was carried out using Scanning Electron Microscopy (SEM) at magnifications of 500×, 1500×, and 3000× and Fourier Transform Infrared (FTIR) in the range of 4000–400 cm⁻¹. The SEM results showed morphological evolution from an amorphous structure to a layered (lamellar) structure; however, the layer orientation remained irregular, and the material was still classified as turbostratic carbon. The presence of porosity and microcracks indicates that the devolatilization process has not been followed by adequate densification. FTIR analysis shows a decrease in hydroxyl (–OH) and aliphatic C–H functional groups and the appearance of aromatic C=C bonds, indicating the occurrence of initial aromatization, but not yet reaching a perfect graphitic structure. Comparison of particle sizes showed that the 5 mm sample underwent a more advanced transformation than the 100 mm sample, although the transformation remained inhomogeneous because of uneven heat distribution. The results indicate that particle size is a key parameter in the carbonization and graphitization processes. Petroleum coke shows potential as a graphite precursor; however, the process conditions used do not meet the specifications for nuclear graphite. An increase in graphitization temperature, particle size control, and further processes such as densification are required to achieve a more regular and stable crystalline structure.