cover
Contact Name
A. Jannifar
Contact Email
polimesin@pnl.ac.id
Phone
+628126930456
Journal Mail Official
polimesin@pnl.ac.id
Editorial Address
Politeknik Negeri Lhokseumawe Jl. Banda Aceh-Medan Km 280 Buketrata, Lhokseumawe, 24301, Aceh, Indonesia
Location
Kota lhokseumawe,
Aceh
INDONESIA
Jurnal Polimesin
ISSN : 16935462     EISSN : 25491199     DOI : http://dx.doi.org/10.30811/jpl
Polimesin mostly publishes studies in the core areas of mechanical engineering, such as energy conversion, machine and mechanism design, and manufacturing technology. As science and technology develop rapidly in combination with other disciplines such as electrical, Polimesin also adapts to new facts by accepting manuscripts in mechatronics. In Biomechanics, Mechanical study in musculoskeletal and bio-tissue has been widely recognized to help better life quality for disabled people and physical rehabilitation work. Such a wide range of Polimesin could be published, but it still has criteria to apply mechanical systems and principles. Exceeding the limitation has been a common reason for rejection by those outside the scope. Using chemical principles more than mechanical ones in material engineering has been a common reason for rejection after submission. Excessive exploration of the management within the discipline of Industrial Engineering in the manufacturing technology scope is also unacceptable. The sub-scope biomechanics that focuses on ergonomics and does not study movement involving applied force on the bio-tissue is also not suitable for submission.
Articles 664 Documents
Analysis of the effect of SMAW welding layer number variation on the microstructure and mechanical properties of the HAZ in ST 41 steel Ratna Dewi Anjani; Ardiansyah Arum; Indra Aditya; Muhammad Ivanto; Rianita Puspa Sari; Deri Teguh Santoso
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9300

Abstract

Welded joints in ST 41 low-carbon steel commonly show unpredictable hardness variation across the Heat Affected Zone (HAZ), and although Post-Weld Heat Treatment (PWHT) and multipass welding are each known to influence this variation, their combined effect on ST 41 has not been systematically examined. This study evaluates how weld pass count (2, 3, and 4 layers) and PWHT at 590 °C interact to affect HAZ and weld metal hardness and microstructure. SMAW welded specimens with E6013 electrodes (Ø3.2 mm) at 100 A. PWHT was applied for 30 minutes, followed by furnace cooling. Dye penetrant testing confirmed all 18 joints were free from critical defects, with minor porosity in three specimens within ASME limits. Without PWHT, the highest mean weld metal hardness was 266.38 HV (4-pass), with an individual HAZ peak of 388.10 HV in specimen T42; the lowest non-PWHT HAZ hardness (239.29 HV) occurred in the 3-pass group. After PWHT, HAZ hardness fell across all pass counts, most markedly in the 3-pass group (196.09 HV, an 18% reduction), although the reduction did not reach statistical significance at the sample size tested. Microstructural examination showed a consistent shift from fine pearlite with poorly defined grain boundaries before PWHT to coarser, more homogeneous ferrite-pearlite afterwards, corresponding with the hardness trend. These results suggest that combining a three-pass sequence with PWHT at 590 °C offers the most favourable hardness reduction for ST 41 weld joints, a finding that warrants confirmation with a larger specimen set.
Design and development of a Karakuri system for cost-effective material transport in manufacturing Benny Haddli Irawan; Esperanda Ivangka Saragih; Adi Syahputra Purba
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.8207

Abstract

In the Industry 4.0 era, optimizing production processes is essential for improving efficiency and competitiveness. Karakuri is a manufacturing automation approach that uses simple mechanical mechanisms powered by gravity and kinetic energy rather than electricity. This study aimed to design and develop an economical Karakuri system for material transport in manufacturing. The proposed system was intended to reduce dependence on manual labor, improve time efficiency, and lower operating costs. The methodology included system requirements analysis, mechanism design, and performance and cost evaluation in an industrial setting. The results showed that the Karakuri system required an initial investment of approximately Rp 6,000,000, compared with Rp 17,000,000 for a conventional electric conveyor. Annual maintenance costs were estimated at Rp 500,000 for the Karakuri system and Rp 1,500,000 for the electric conveyor. Over three years, the reported total cost of ownership was Rp 7,500,000 for Karakuri and Rp 37,700,000 for the electric conveyor, representing an estimated cost reduction of approximately 80%. The Karakuri system also operated without external electrical power. These findings indicate that Karakuri offers a cost-effective alternative for material transport in manufacturing, particularly for companies seeking to reduce investment and operating costs.
Effect of carbon volume fraction on the electrical conductivity and the porosity of carbon–ceramic composites for hair straightener heating elements Hawa Rizka; Agus Edy Pramono; Ahmad Maksum; Nanik Indayaningsih
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.7176

Abstract

The advancement of hair straightener technology has increased the demand for heating materials that not only exhibit high electrical conductivity but also maintain structural stability. Conventional metal-based heating elements present several limitations, including susceptibility to corrosion and limited mechanical flexibility, making carbon–ceramic composites a promising alternative. This study aims to develop a carbon–ceramic composite material as a heating element for hair straighteners by varying the carbon volume fraction at 10%, 20%, and 30%. Coconut-shell-derived carbon was employed as the conductive phase, while a ceramic matrix was formed from a mixture of clay, kaolin, feldspar, and silica sand. The composite samples were fabricated using a sintering method at a temperature range of 930–950 °C. The materials were characterized in terms of their electrical and physical properties, including electrical conductivity, porosity, density, and compaction pressure. Results showed that increasing the carbon fraction significantly enhanced the electrical conductivity from 8.60 × 10⁻⁶ S/m at 10% carbon to 3.83 × 10⁻³ S/m at 30% carbon. However, higher carbon content also led to increased porosity and reduced density, which may negatively affect the mechanical strength of the material. Therefore, optimizing the carbon-to-ceramic ratio is essential to achieve a balance between electrical efficiency and structural integrity, particularly for heating applications such as in hair straightening devices.
Real-time OEE monitoring system integrating Odoo MRP and Omron NB HMI via Modbus TCP for an induction heating machine Gun Gun Maulana; Siti Aminah; Nur Wisma Nugraha; Arya Sangaji; Tyarakusuma Emirae
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9667

Abstract

Induction heating machines are critical production assets, yet their performance is often monitored manually through local HMI panels. This practice can delay Overall Equipment Effectiveness (OEE) reporting and introduce inaccuracies. Existing real-time OEE architectures for Odoo-based MES platforms have not been demonstrated on induction heating equipment. In such installations, standalone HMI panels remain disconnected from centralized OEE systems, leaving operators dependent on delayed and error-prone manual reporting. This paper presents the design and implementation of a real-time OEE monitoring system integrating Odoo 18 MRP with an Omron NB HMI via direct Modbus TCP communication, without intermediate middleware. The system comprises three custom Odoo modules: mrp_oee_custom (OEE engine and REST API), mrp_oee_modbus (Modbus TCP I/O and state machine), and mrp_shopfloor_custom (shop floor monitoring). The core mrp_oee_modbus module uses a background polling thread, with a cron-based fallback, to read six HMI registers and write OEE values to 24 output registers. This enables operator-level OEE display without browser access. System reliability was evaluated through a 26-day uptime test (130 operating hours) and 12 fault-injection scenarios. Communication performance was assessed by analyzing 26,040 Modbus TCP transactions from three Wireshark capture sessions. Functional correctness was verified through 14 Odoo and 10 HMI black-box scenarios, while OEE calculation accuracy was validated across five production runs. The results showed: uptime of 99.69%, an MTBF of 32.4 hours, an MTTR of 6 minutes, a 100% auto-recovery rate, mean Modbus TCP latency of 5.92 ms with 0.00% packet loss (P99 = 33.4 ms, jitter:4.99 ms), and 100% functional test pass rate. OEE calculations deviated from manual calculations by a maximum of 0.005 percentage points (mean deviation: −0.001 pp). This error is substantially below the 1-percentage-point resolution commonly used for OEE-based production decisions and therefore has negligible practical impact on monitoring accuracy.
Joint strength and electrical resistance of AA6201/copper joints produced by rotary friction welding Yeni Muriani Zulaida; Mahfudz Al Huda; Kirman Kirman; Hermawan Agus Suhartono; Muhammad Anis
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9857

Abstract

Aluminum alloy 6201 (AA 6201) is widely used in electrical applications due to its excellent electrical conductivity and lightweight characteristics. To enhance its industrial applicability and added value, dissimilar joining between AA 6201 and copper has attracted considerable interest, particularly for electrical connector systems. In this study, rotary friction welding was employed as a solid-state joining technique capable of producing high-quality dissimilar metal joints while minimizing defects commonly associated with fusion welding processes. However, the formation of intermetallic compounds at the Al/Cu interface remains a critical issue, as these phases may improve joint strength but simultaneously deteriorate electrical conductivity. This research comprehensively investigates the effect of rotary friction welding parameters on the mechanical strength and electrical resistance of AA 6201/Cu dissimilar joints. Friction time was varied to evaluate their influence on joint characteristics and plastic deformation, as indicated by the amount of aluminum metal transferred to the copper surface. Moreover, the joints exhibited excellent mechanical performance, achieving a joint efficiency of up to 100%. Electrical resistance measurements showed that the Al/Cu joint exhibited lower electrical resistance, corresponding to higher electrical conductivity than the AA 6201 base metal, with the electrical resistance reduced by up to 60%.
Effect of hybrid reinforcement and heat treatment on phase evolution, microstructure, and hardness of Al6061/SiC/MWCNT/graphite composites Atik Setyani; Muhammad Syukron; Ibnu Cahyo Nugroho; Agris Setiawan
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.8904

Abstract

The development of lightweight and high-strength materials is increasingly important for transportation and aerospace applications. Al6061 is a promising structural alloy; however, its mechanical performance can be limited by microstructural heterogeneity and the distribution of strengthening phases. Although SiC, carbon-based reinforcements, and T6 heat treatment have been individually investigated in Al6061 composites, the combined response of SiC/MWCNT/graphite hybrid reinforcement to T6 treatment, particularly in terms of phase evolution, microstructural distribution, and hardness, remains insufficiently understood. This study investigated Al6061 hybrid composites reinforced with SiC, MWCNTs, and graphite produced by stir casting and subsequently subjected to homogenization, solution treatment, rapid quenching, and artificial aging. Microstructural and phase characterization was performed using optical microscopy, SEM-EDS, and XRD, while hardness was evaluated using the Rockwell B scale. The untreated composite consisted primarily of an α-Al matrix containing Mg2Si and dispersed reinforcing particles, although localized graphite agglomeration was observed. Heat treatment promoted a more homogeneous microstructure and modified the distribution of Mg2Si precipitates. XRD confirmed the presence of FCC α-Al, Mg2Si, and reinforcement-related phases. The heat-treated composite exhibited the highest hardness of 48.28 HRB, compared with 45.22 HRB for the untreated composite and 22.68 HRB for unreinforced Al6061. The hardness improvement is attributed to the combined contributions of hybrid reinforcement and precipitation strengthening. These results demonstrate the role of T6 heat treatment in tailoring the microstructure and hardness of Al6061/SiC/MWCNT/graphite hybrid composites.
Mechanical performance of SLA-printed BCC, FCC, and hexagon lattice structures under various layer thicknesses and post-curing times Candra Irawan; Agus Sifa; Tito Endramawan; Dedi Suwandi; Muhammad Luthfi; Emin Haris; Ahmad Farhan; Claudha Alba Pradhana
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9936

Abstract

The mechanical performance of stereolithography (SLA)-printed lattice structures is governed by both unit-cell topology and processing parameters. However, previous studies have largely examined lattice topology and SLA processing parameters separately, with limited systematic investigation of their combined effects on manufacturing quality, mechanical performance, and structural efficiency within a unified experimental framework. This study experimentally evaluated three lattice topologies, namely Body-Centered Cubic (BCC), Face-Centered Cubic (FCC), and Hexagonal, combined with layer thicknesses of 0.05, 0.10, and 0.15 mm and post-curing times of 40, 50, and 60 min. Five specimens were tested for each of the nine Taguchi L9 experimental conditions (n = 5), and the responses were analysed using the Signal-to-Noise (S/N) ratio and Analysis of Variance (ANOVA). Manufacturing quality was evaluated from dimensional accuracy and mass, while mechanical performance was assessed through Shore D hardness and tensile, compressive, and flexural tests. Structural efficiency was evaluated using Mass Reduction (MR), Mechanical Performance Retention (MPR), Specific Mechanical Performance (SMP), and Mechanical Performance per Apparent Volume (MPV). The BCC topology exhibited the highest dimensional accuracy, with a strut diameter deviation of 0.60%, whereas Hexagon showed the largest deviation of 7.60%. Layer thickness was the dominant factor affecting hardness, contributing 97.8% of the variation, while lattice topology dominated tensile, compressive, and flexural strength, with contributions of 89.7%, 91.6%, and 55.8%, respectively. FCC provided the highest MPR, SMP, and MPV values, whereas Hexagon achieved the highest mass reduction of 26.50%. Within the investigated parameter ranges, FCC with a 0.05 mm layer thickness and 40–50 min post-curing provided the most favorable overall performance. These results demonstrate that integrating lattice topology, SLA processing parameters, mechanical performance, and structural efficiency provides a comprehensive basis for selecting lightweight lattice configurations.
Effect of electrode dressing on weld nugget diameter and electrode life in automotive resistance spot welding of galvanized steel Habib Rizqon Halala; Annisa Bhikuning; Triyono Triyono
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9484

Abstract

Resistance spot welding (RSW) is widely used in the automotive industry because of its high productivity and ability to produce reliable sheet-metal joints. However, electrode-tip degradation during galvanized-steel welding can reduce weld nugget diameter and compromise joint quality. This study investigates the effect of electrode dressing on nugget diameter and estimates electrode life during RSW of 1.1 mm JAC270DN-45/45 galvanized-steel sheets. Weld quality was evaluated using ultrasonic non-destructive testing at four weld counts (1, 150, 250, and 400) with a dressed electrode and seven weld counts (1, 50, 100, 150, 200, 250, and 400) without dressing. Nugget diameters were assessed against the 4.5 mm minimum requirement specified in JIS Z 3140 for the investigated sheet thickness. With electrode dressing, nugget diameters remained between 9.4 and 8.7 mm, and all measured welds met the acceptance criterion. Without dressing, nugget diameter decreased with increasing weld count and reached 4.15 mm at the 400th weld, below the required minimum. Regression analysis estimated a usable electrode life of approximately 339 welds without dressing. These results indicate that electrode dressing helps maintain nugget diameter and weld quality during galvanized-steel spot welding. The estimated electrode life is specific to the tested material and welding conditions.
Experimental investigation of inclination angle and working fluid effects on the thermal performance of a CLPHP I Wayan Sugita; Ragil Sukarno; Rangga Bagus Santosa; Ferry Budi Susetyo
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9099

Abstract

The growing demand of energy-efficient thermal management systems has increased the need in compact heat-transfer devices such as the Closed-Loop Pulsating Heat Pipe (CLPHP). This study experimentally investigates the effects of inclination angle, heat input, and working fluid on CLPHP thermal performance. A copper CLPHP with a 2 mm inner diameter, five turns, and a 65% filling ratio was tested at inclination angles of 0°, 30°, 45°, 60°, and 90°, using distilled water and ethanol as working fluids. Heat input was ranged from 10 to 50 W. The primary parameters analyzed were thermal resistance (Rth) and heat transfer rate (Qout). The results showed that thermal resistance generally decreased as heat input increased, although a slight increase occurred for ethanol at a horizontal orientation under certain conditions. The minimum thermal resistance was 0.24 °C/W for distilled water and 0.60 °C/W for ethanol, both at 50 W and 60°. The maximum heat transfer rate was 47 W for distilled water at a 90° inclination. These findings indicate that CLPHP performance depends on the combined effects of heat input, inclination angle, and working-fluid properties. Distilled water provided lower thermal resistance under the tested conditions, while the inclination associated with the best performance depended on the selected performance indicator.
Additive manufacturing in UAV development: a review of processes, materials, mechanical performance, and component applications Muhammad Ikhlas; Mohammad Zaini Ma'ruf; Yasya Khalif Perdana Saleh; Nurul Jumiati; Taufik Kurniawan; Abubakar As'siddiq; Fakhril Husain
Jurnal Polimesin Vol 24, No 5 (2026): October
Publisher : Politeknik Negeri Lhokseumawe

Show Abstract | Download Original | Original Source | Check in Google Scholar | DOI: 10.30811/jpl.v24i5.9064

Abstract

Unmanned Aerial Vehicles (UAVs) increasingly require lightweight structures, complex geometries, and high functional efficiency, while conventional manufacturing is constrained by geometric limitations, lengthy assembly, and high tooling costs. Additive Manufacturing (AM) offers an alternative through layer-by-layer fabrication, design flexibility, and reduced material waste. This review examines the role of AM in UAV fabrication by comparing five principal AM routes: Fused Deposition Modeling (FDM), Selective Laser Sintering (SLS), Stereolithography (SLA), Selective Laser Melting/Laser Powder Bed Fusion (SLM/LPBF), and Directed Energy Deposition (DED). The review evaluates the relationships among manufacturing process, material system, mechanical performance, and UAV component requirements, including lightweight design, geometric complexity, rapid prototyping, and low-volume production. The findings indicate that FDM with continuous carbon fiber reinforcement is well suited to lightweight structural frames and landing gear, while SLS using PA12 is advantageous for geometrically complex polymer components. SLA is suitable for precision mechanisms, whereas SLM/LPBF using titanium alloys is more appropriate for high-strength brackets and load-bearing components. DED is mainly applicable to repair and large-scale metallic fabrication. However, limitations including anisotropy, process sensitivity, dimensional variability, and limited operational validation remain important challenges. Overall, no single AM process satisfies all UAV requirements. Process selection should therefore consider component function, material behavior, mechanical loading, and service conditions. By mapping these interdependencies, this review provides a structured basis for evidence-based AM process selection and highlights future research directions for reliable UAV development.